Re: Brand?
Brian Roberts
Thanks John.....
I wondered if you were using a pre-cat finish.
No finish (that I know of) that depends on solvent evaporation will be buff-able in the short time you spoke of.
One major advantage....IMHO... to nitrocellulose is the ease of repair....subsequent coats dissolve the previuos coats resulting in one thicker layer.
Sanding between coats is not necessary for bonding....although may be desired for leveling.
During my stint in a cabinet shop we used exclusively pre-cat lacquer.
It was great for putting a quick and very tough finish on cabinets.
We made VERY sure we would not have any reason to go back later and do any sanding for leveling....it was way too easy to sand thru a layer of the pre-cat........the ghost rings were impossible to eliminate.
It was a pita for clean-up and smelled far worse....thankfully we had a good spray booth.
For my (home shop) purposes pre-cat finish doesn't make sense.
My experience with guitar manufacturing involved dealing with many different finishes and mixtures of those finishes. An amazing amount of testing and research went into trying to develop the "perfect" formula for nitrocellulose lacquer. Varying the formulas to increase hardness, decrease dry time, improve flow-out, etc, etc.. A change made to improve one quality almost invariably had a negative effect on another.
Several guitar companies, working with the top finish companies, worked on it for years.....and probably continue to I am quite sure.
Taylor Guitars was the forerunner in developing a UV cured system of finishing for musical instruments. The change to UV cured finish became a necessity....to solve the huge bottleneck that was caused by the long cure times for the "old" finishes. I believe the banning of nitro finishes in California was, at that time, "just around the corner".....which was further impetus for change.
The company I worked for switched to a UV cured "system".....which definitely came with a "learning curve"....and touch-up was......well......a very real PITA....
I guess the bottom line is that there is no perfect finish....for all applications.