Premature polymerization: another solution?

mjonesrdg

So, I got it... that it was not entirely a "storage" problem with the finishes skinning over or gelling in the jar. Solutions to that concern, including the marbles, the water-on-the-bottom, the Bloxygen*, the squeezed can, etc.,did not address the concern of presenting the air to the container with each opening, use, and closing again. If I were to put five coats of oil/varnish on a 12" diameter form, I'd open the container five times to retrieve something less than 1/2 ounce of finish. Multiply this by 10 similar forms, fifty exposures to the air would ensue.

I ordered a dozen of these 'Cath Syringes' last spring. Initially, the concept failed, to a degree, because a small amount of air got pushed back into the syringe when I put the cap back on. Shown here, with a push pin in the cap, I can force ALL the air out, and I have not lost a drop of finish since. This "test period" time is short and not conclusive, but my summers are hot and my shop not insulated. It holds good promise.

An unexpected benefit came from the graduation markings on the syringe body. Very helpful when measuring the ingredients of my "home brew" wipe-on varnishes.

At about 2 bucks each, and reusable, I might get all the way through a quart of finish before the premature polymerization foils me again.


img

Re: Premature polymerization: another solution?

#2

Roger in MO

Re: Premature polymerization: another solution?

Roger in MO

I like the idea. I wonder if a plastic veterinary syringe available in farm stores would work with a modified needle. I'll buy a couple the next trip to town.

I currently am using MinWax oil stored in a full halfpint fruit jar for over a year in a refrigerator but once opened its difficult to seal again and now has at least 1/2 inch of air space at the top.