Posts

Re: Bad Picture of a Little Box

#26

Re: Jen -Talk to Bob Coogan

Jennifer Indy.USA

Hey John,

We'll be down there in July. Maybe I'll see if there's any left. I wonder what gauge that stuff is? I've been using 18g but am wondering what 20 would be like?

Jen

Re: Bad Picture of a Little Box

#27

Steve Kubien

Re: Jen -Talk to Bob Coogan

Steve Kubien

Ummm, thinner? No?

Runnin' and duckin'

Re: Bad Picture of a Little Box

#28

Re: Bad Picture of a Little Box

charlie belden

If you have a junior college, college or university nearby, they may have jewelry classes. If they do, they usually get a bookstore to carry copper, nickle silver, silver and brass sheet stock.

Re: Bad Picture of a Little Box

#29

Re: Jen -Talk to Bob Coogan

John Lucas

I may see him Thursday, I'll try to remember to ask. It was pretty thick I think.

Re: Bad Picture of a Little Box

#30

Re: Roofers

bill johnson

You are so right Jorge and it is available the last time I checked at the orange box it's available in rolls called flashing. It may have an easily removable backing on it.

Re: Bad Picture of a Little Box

#31

1/32"

Jorge Casta�eda

Jen,

Don't remember the number but the copper we use is 1/32".

Re: Bad Picture of a Little Box

#32

But....

Bill Howatt

... you'll only get 98 for every 100 US pennies (neglecting fees) and what's worse they aren't pure copper anymore either! :)

Bill

Re: Bad Picture of a Little Box

#33

Copper thicknesses and etc.

Dale Miner

To confuse things, or rather, interject the existing confusion:

Roofing copper is measured in ounces. That is, how many ounces a square foot of it weighs. So, in roofing copper, the higher the ounce rating, the thicker it is. 16 ounce copper is about .0216 inches thick, 20 ounce copper is about .0270 inches thick. Those are two of the common thicknesses used in roofing work.

Sheet gauge is a different story. The higher the gauge number, the thinner the sheet is. 18 gauge copper is .0403 inches thick, almost twice as thick as 16 ounce copper, and 16 guage copper is .0508 inches thick. Copper that is 1/32 inch thick (.0315") is about the same as 20 gauge at .0320 inch, and will weigh 23.74 ounces per square foot, and would be roughly equivalent to 24 ounce copper at .0323 inches thick. 32 ounce copper is .0431 inches thick, and 32 gauge copper is .0080 inches thick. Confused yet? I have the book in front of me and I am.

Roofing copper comes with either a soft temper or a 1/8 hard temper and is ASTM B 370. Another grade of copper sheet is ASTM B 152 Alloy 110 Electrolytic Tough Pitch. It comes in gauge thicknesses in either an annealed soft temper or a half hard temper.

Both grades are essentially pure copper with similar mechanical properties in the annealed or soft temper state. Both grades will work harden rapidly. The ASTM B 152 Alloy 110 'might' have slightly better drawing qualities. Doubtfull that if there is a difference, it would be noticeable unless the material is worked extensively. If anything other than a simple shape or pattern is planned, it is best to start with the annealed soft temper.

For metal spinning, I use 20 ounce roofing copper, soft temper, and anneal frequently. Annealing is accomplished by heating until a dull red is seen with the shop lights dimmed. The material can be but does not need to be quenced in water. Quenching in water helps to break the oxide layer and make it easier to remove. The oxide scale can be removed with a pickling solution containing sulfuric acid, or by abrasion. Working the material without removing the scale will cause the scale to become imbedded in the material.

Heating to a higher heat than needed, or holding the material at a red heat for prolonged periods is detrimental to the process. Oxides will form at the grain boundries and degrade the working properties as well as leave oxide inclusions in the material. I generally try to quench the material as soon as possible after annealing temperature has been reached to help in scale removal and minimize the time the material is hot enough for oxides to form.

Re: Bad Picture of a Little Box

#34

Leo Cuellar

Re: Railroad tracks make great small anvils

Leo Cuellar


A friend made this one. Its a little rough but works for basic beating. Even has a hardy hole.

Re: Bad Picture of a Little Box

#35

Re: Actually.......

Malcolm Ray

Jen, Most lumber yards carry copper flashing in rolls of different widths,they sell it by the foot or the pound,you can cut any length you want off a roll....not that expensive......you can also buy it in 30" and 48" wide sheets..........I used it for the roof on a couple of my cupolas, and a bay window,its worth the cost

Re: Bad Picture of a Little Box

#36

Re: Copper thicknesses and etc.

Jennifer Indy.USA

Dale, thanks for this info. I've been over heating my copper. Would a swimming pool supply store have muratic acid?

Jen

Re: Bad Picture of a Little Box

#37

Re: Copper thicknesses and etc.

Don at Central Illinois

Ace Hardware should care Muratic Acid. It's used for cleaning up concrete.

Re: Bad Picture of a Little Box

#38

Thanks Don!

Jennifer@Indy.USA

Re: Bad Picture of a Little Box

#39

Flux!

charlie belden

Borax powder - in alcohol - makes a great thin coat layer of flux. Alcohol evaporates immediately on the piece, leaving a thin layer of borax on the whole metal surface. It melts before the copper gets hot enough to start absorbing oxygen and sticks around long enough for you to anneal the copper. You can brush it on or immersed the piece in the alcohol borax suspension.

Might want to pick up some "pickling" - dry granular material which, when dissolved in hot water will remove oxidation on metal. Check jewelry suppliers. A small crock pot with lid and with pickling solution is usually found on a jewelers work bench - or at a soldering station.

Re: Bad Picture of a Little Box

#40

Re: Flux!

Jennifer Indy.USA

Have you tried this....or did you read it somewhere? I'm wondering if there are any bad off gasses or other negatives to using this over muratic acid. The thought of having either sitting on my bench doesn't excite me! I was going to pic up some muratic acid today.

Jen

Re: Bad Picture of a Little Box

#41

Steven Antonucci

Blacksmiths use "flux" all of the time

steven antonucci

I use a granular material labeled "flux" all of the time to prevent oxides from forming when I am atempting to forge weld (notice the word attempting... I am still not good at it...)

A flux is merely a barrier to prevent the oxide from forming and I assume that there would be something that prevented the companies from selling it if it were hazardous? The can that I have make no mention of any bad gases, and like Charlie said, forms a barrier just long enough to keep your metal from going black.

Steve

Re: Bad Picture of a Little Box

#42

Re: Flux!

John Veerkamp

Muriatic Acid is by far the more toxic substance. Borax is fairly benign and is often used as a laundry additive. We've used it for years with no issues. No odor or residue on the clothes. In solution it does not irritate the skin either. It would be my choice.

Re: Bad Picture of a Little Box

#43

Re: Flux! Thanks!

Jennifer Indy.USA

thanks guys!

Re: Bad Picture of a Little Box

#44

Re: Flux! It's safe because? HUH?

Don Evans

There are a lot of assumptions being made here based on totally different uses of a product which can and some times does lead to false conclusions.

The fact for example that mixing borax with water and using it in that solution doesn't necessarily make it safe when NOT mixed and heated directly with a torch!

I'm NOT saying it is harmful, I really don't know, but I do know this. Anytime industrial plants do this stuff they have vent fans to the outdoors to take the gasses created by the excessive heat away from the worker.

Heating acids, & other things, with a torch could give off toxic gasses and for safety you should always assume that what you are doing, when a torch is involved, will harm you. Never breath the fumes and never do it in an enclosed space without adequate outside ventilation.

Re: Bad Picture of a Little Box

#45

Steven Antonucci

FYI- 20 Mule Team Borax at the grocery store

steven antonucci

Might be a cheap way to try.

Steve

Re: Bad Picture of a Little Box

#46

Re: Flux!

Doug Trembath

Jen, just a quick heads-up, but if you use Muriatic acid, do it outside the shop. The fumes will, if given the opportunity, cause rust to form on any exposed steel or iron surfaces. This has been reported quite a bit on forums and discussion groups here and in other places.

Doug Trembath

Re: Bad Picture of a Little Box

#47

Re: Flux!

charlie belden

I did lost wax cast jewelry and small sculpture and taught it through adult ed for about 12 years. The alcohol / borax suspension is not hazardous at all - unless you and it are confined in a small air tight space - in which case breathing the alcohol fumes would give you a headache - the borax powder in suspension doesn't make it into the air. The alcohol is merely a medium to get a thin layer of the borax to coat the surface of your metal. It has a much lower melting point than the annealing temperature of copper and most other metals jewelers use. It will become a liquid that covers your metal and keeps oxygen from getting to it - assuming you don't keep the torch flame on the metal for several minutes at or above the annealing temperature

Borax was, and may still be, used in laundry detergent. Ronald Reagan was the spokesman for "20 Mule Team Boraxo" laundry detergent. Unless you were to swallow a bunch of it, snort it or shove it in your eye - it's pretty harmless. It can be mixed with water and gum tragacinth to make a thicker paste you can brush on, but if you heat it with a torch while still wet, the water will boil and the paste will bubble. For your application that might not be a problem. But if you have small snippets of silver or gold solder that you want to place - and keep it there 'til it flow and solders parts together, bubbling flux usually moves your snippets around - for some reason always away from where you want it to be.

If you use the paste thick flux, borax or other chemical as the key ingredient, you'll have some of it melted on you metal that you'll have to remove - usually by dissolving it in a "pickling solution" you quench the piece in. Sometimes quenching just in water will knock it off. BUT a thin layer of borax, melted on your now annealed metal often doesn't even require pickling.

Now if you want to CLEAN the surface of a piece of metal, a hot cyanide and water solution was, and probably still is a jewelers first choice, assuming there's no steam cleaner available. But that's another story and you'll probably never need it.

I can hunt up my jewelery making books and send you a few if you want to pursue playing with non-ferrous metal. Don't know if Oppi Untracht's book is still in print but it's pretty comprehensive. Shar Choate also wrote a pretty good book on jewelry making as well.