Purpleheart

Eric Knutsen

I plan to use purpleheart for 2 turnings- a pen and letter opener. I will be doing a CA finish. My question is, after sanding should I simply go right to the CA or use some kind of oil first?

Re: Purpleheart

#2

Re: Purpleheart

Bruce Pratt

Straight to CA is fine, however, wait a couple of days for the purple color to re-appear on the surface of the wood before applying the CA. It will look brown immediately after turning.

Re: Purpleheart

#3

Re: Purpleheart

John Lucas

It will still turn purple when subjected to sunlight even with a finish. It will just take a few days longer.

Re: Purpleheart

#4

Re: Purpleheart

Craig Daymon

Oil on Purpleheart would not be a good choice as it would tend to speed the purpleheart in turning brown. Also, it may impact the ability of the CA finish to attach to the surface. CA is essentially a dissolved acrylic. When the solution in which it is dissolved evaporates, which it does very quickly, you are left with an acrylic finish.

Best to stick with just the CA, though I agree with letting it wait a day before applying the finish. I personally believe the purple color comes more from an oxidation effect than from sunlight as I have turned and sanded piece, left them in a dark room and come back the next day to find the color bright purple, as opposed to the duller, browner, color present after sanding. I believe the slower change to purple that John has reported after applying CA is because CA (and pretty much any finish) will still let oxygen get in.

That last paragraph is my opinion based on my experience. Others are welcome to theirs.

Re: Purpleheart

#5

Re: CA

Bruce Pratt

Craig, not to get too particular about it, but the liquid CA in the bottle consists primarily of monomers of cyanoacrylate which rapidly polymerize in the presence of water to form the hard plastic finish. There may also be carrier solvents in the liquid CA. If present, however, their evaporation would not measurably contribute to the creation of the polymerized plastic finish.

Re: Purpleheart

#6

Re: Purpleheart

John Lucas

Craig Oxidation could be part of the process but if I make a lidded box and set it aside in the sun the outside will change to purple and the inside will take months and months to change unless I put it in the sun. So I don't really think Oxidation is the sole answer. Same is true with Box elder. Open one of my older box elder boxes and the inside will still be bright red. The outside that hasn't been in direct sunlight will have lost some color. I don't think my box lids are airtight. :)