Sea Urchin Treatment

Stuart Johnson

What finish works well on Sea Urchin ornaments, possibly colored but more than likely clear?

Re: Sea Urchin Treatment

#2

Re: Sea Urchin Treatment

Bill Howatt

I don't put any finish on the shell part.

Bill

Re: Sea Urchin Treatment

#3

Re: Sea Urchin Treatment

Craig Daymon

I just finished my first of these this year. The top cap and finial were made from Jatoba closest to the shell and some kind of rosewood (with a really neat grain pattern - maybe Kingwood?) for the longer part of the finial and for a bead on the top cap. I sanded al the wood parts to 1500 and connected it all together with a center dowel, rather than gluing to the shell.

I just finished the wood parts with Conservator's Wax. Looks really good. (Bias applied, of course.) Conservator's wax is a microcrystalline wax that is not suppose to show finger prints and you only need to use a little bit.

Re: Sea Urchin Treatment

#4

George Balock

Re: Sea Urchin Treatment

George Balock

Stuart,

I generally finish the cap and finial with Behlen's Woodturner's wipe on finish. These parts are typically made from some exotic that likes that finish. I then finish the shell with Krylon Acrylic, matt or gloss depending on my mood.

George

Re: Sea Urchin Treatment

#5

Stuart, Ed Moore showed us how to....

JamieDonaldson

...strengthen the shells with Krylon Triple Thick Crystal Glaze, and it works well.

Re: Sea Urchin Treatment

#6

Re: Stuart, Ed Moore showed us how to....

Phillip Medghalchi

Stuart, where are the pic.s. they sound nice, we would like to see pic.s.

Re: Sea Urchin Treatment

#7

Mike Stafford

Ed Moore strengthened the shells with...

Mike Stafford

Triple Thick Krylon glaze but finished with spray lacquer.

If you wish to dye the shells I have had more success dying first with aniline alcohol dyes followed by the Krylon glaze and finally the lacquer.

The shells are very porous so you have to be careful about your dye strength.