CA is not my friend
Mike Foster
Some here might remember me dissing CA before. My original reason for this is that I learned more about the chemistry of CA. A Smithsonian conservator discussed CA with Steve Sinner and mentioned that it was a glue that is not at all archival. The CA is accelerated by exposure to water, which is why you can actually spritz CA with water as an accelerator. Not sure what is in the commercial accelerators, but I would bet they are largely water, although they do have a chemical smell. Problem is that the cured CA keeps reacting with exposure to water over time (although much slower) and will eventually turn into dust. So the Smithsonian folks strongly discourage the use of CA in any work that wants to last any length of time. I am sure the rate is affected by all sorts of things, including top coats of other finish.... but the fact remains, eventually dust.
All that has nothing to do with this post though. I bought a bottle of CA from an unnamed distributor that claims purity and excellence. They tend to promote buying in larger quantities. Well I bit on it a couple years ago and bought a 12 oz (or so) bulk bottle. I store this on the shelf with all my other glues ( although it was living in my freezer for a while). I went to get some epoxy a few days ago and found that the whole dang shelf was flooded with CA about 1/4" deep. It was about 1/2 cured. To top this off, I had been using the CA recently and found that it wouldn't cure completely for over 1/2 hr. I chalked that up to perhaps being out of date. Well, I did not inspect the bottle the CA came in as it was obvious it leaked because it was standing upright on the shelf. Spent about 45 minutes this evening cleaning up the mess. Some cured that needed to be chiseled off, some only partially cured that needed to be scraped off and cleaned with acetone. Should have put on a respirator, but just couldn't be bothered and tried to keep from breathing the fumes as much as possible.
So you can be sure I will never buy CA from the unnamed supplier again and never in bulk. I actually still use CA some, but really only very rarely. I always try to come up with a better alternative. Let me just say that I really don't understand the folks that use CA as a finish. In my opinion, there are much better alternatives. OK, now I feel better.
First time I saw CA was at Plattsburgh AFB in 1976. They were using open pint bottles and applying it to the repair the honeycomb sections inside of the wing. I got a bottle and took it back to the Fire Station. Had lot's of fun seeing what could be glued together... Glued some quarters to the stall floors, funny watching people try to pick them up...