Mahoney's Walnut Utility Finish
Stuart Johnson
How long does it take for this to cure indoors around 70 degrees?
Knowledge You Can Build On — Est. 1998
Mahoney's Walnut Utility Finish
Stuart Johnson
How long does it take for this to cure indoors around 70 degrees?
Re: Mahoney's Walnut Utility Finish
John Lucas
I have my house set at 70 and it seems to dry overnight. I apply a new coat each day when I use it.
Re: Mahoney's Walnut Utility Finish
Bernie Weishapl
After 2 or 3 coats I let them dry for a week and I always put them where there is a lot of sunlight since Mike told me at one of his demo's that sunlight helps cure it.
Re: Mahoney's Walnut Utility Finish
Joe Fleming
What Bernie said. Also, do not submerge the piece in the oil. If you saturate the piece it will take forever to dry. Wipe on and wipe off. Joe
Re: Mahoney's Walnut Utility Finish
robo hippy
I slop it on, let it sit for an hour or so while I sand and finish another bowl or three, then wipe on some more. I prefer to let it sit for a day or two, then a final wipe down. It does take a week or so to cure to the point where it won't leave oil rings on the table cloth, but is dry to the touch in a day or so. I have sped the process up by putting the bowls on a wire rack over a 40 watt bulb.
robo hippy
Thanks for the replies.
Stuart Johnson
It sounds like the best thing to do is set the bowl aside for a week and let it cure. I do like the soft look the oil gives.