GaryG in MD
I've started making a few pens, and I'm trying to make them look different from each other. I finished the first couple with Hut Crystal Coat, which yellows the wood. I don't want them all looking yellowish. So I figured I'd try one with water-based poly. I read the back of the can carefully, and amidst all the directions and warnings, it says to sand the first coat back at 220 to make sure the second coat sticks. They don't say anything about the sanding level of the wood before the first coat. I have already sanded the wood to 4k, and I don't like the idea of going back to rough it up again.
So, finally, my questions is: will water-based poly stick to wood sanded to 4k, or will it decide to peel or flake or wear off sometime later? Pens obviously get a lot of rough use, so this would be a kind of acid test for a finish.
I'm sure some of you must have experience with this kind of thing.
Thanks, Gary