Bob Moffett

Russ' finish

Bob Moffett

I wnat to mix up some of Russ' finish and wanted to know if I have the formula correct. Is it 1/3 Mineral Oil, 1/3 gloss polyurethane and 1/3 tung oil? What are the best brands to use. Is their something comparable that is already mixed up and avaliable? What do ya'll think of this finish? I have been using Waterlox, but have trouble with it jelling.

Re: Russ' finish

#2

Not Russ' finish

Mark Mandell - Gone Round In Jersey

Check the Russ' Corner article section. I'm pretty sure you'll find he used 1/3 varnish, 1/3 terps, and 1/3 tung oil [no mineral oil].

Re: Russ' finish

#3

Re: Russ' finish

Vince Welch

Hi Bob,

This is the finish I have been using for years (no mineral oil). I using it because like you I used Waterlox but did not like the jelling. This formula has been around for years and works great. What I like about it is the cost is reasonable and so I do not have to use it sparingly. I put some really good coats on and wipe it off. After 3-4 coats depending on the project I always seem to get the nice sheen that I am looking for. I like a polished look but not a real high gloss finish look. I like the wood to speak for itself per say. Also on smaller pieces you can submerge the piece in the finish. Any buffing that is done really allowing the wood grain to pop.

Vince

Re: Russ' finish

#4

Re: Russ' finish (NEVER mineral oil)

mjonesrdg

Two suggestions from one who has been a home brew varnish tweaker for the last roughly three years. First: Knowing that the proportions are not laboratory- level-critical, it will still be helpful from the get-go for you to measure the ingredients and record your recipe. In cold weather, use more thinner...for that last coat increase the varnish, and decrease the thinner and oil. Measuring spoons work just fine and a twelve inch bowl can be coated inside and out with three tablespoons of mix,

Second: the surface that you put your first coat on should be glass smooth, with no open grain/no visible tool marks, no sandpaper scratches. Achieve this with lacquer or shellac sanding sealer(as needed). In other words it should be perfectly finished before you begin applying your finishing coats of oil.

The tung oil and thinner have a very long shelf life. Your varnish should be kept out of contact with the air. McClosky's Man-O-War is one of the best and can be found wherever paint supplies are sold and it comes in gloss, semi-gloss, and satin. You can lay-up a deep,rich, finish without a glossy glare with subsequent coats.

It is my opinion that no mineral oil, no vegetable, or nut oil should be substituted for the tung oil. Boiled linseed oil could be used in place of tung oil, but it will tend to yellow over time...tung oil will not,

Mike Jones in Redding CA

Re: Russ' finish

#5

Re: Russ' finish

Bill Neddow

I agree with Mark. Use turpentine. Also, you should always use spar varnish. The newer polyurethane varnishes will turn yellow very quickly, just like linseed oil. (see point 7. on Varnishes in Russ' Corner). This finish, made with tung oil (make sure it is the real stuff like the Lee Valley product), spar varnish (which has NATURAL resins) and turpentine, is an ancient formulae that will stand up to use outside as well as inside the house. Thus, you can wash the bowl without fear that the finish will be effected. I use this all the time. When I get lazy, I will use Behlens Salad Bowl finish, which is the same thing, only more expensive.

Re: Russ' finish

#6

Re: Russ' finish

Greg Haugen

Russ brought this finish to the turning community. Sam Maloof also used a "1/3's" finish on his rocking chairs for decades. I'm not sure if Sam's was thinned with Turp. or mineral spirits.

One thing is for sure, it works very well.

Re: Russ' finish

#7

Steve Kubien

Re: Russ' finish

Steve Kubien

'Tis an old way of finishing. Before I discovered lathe work and still thought the Earth was flat and square, this was called "witches brew" by loads of handtool junkies. Not sure I would like it on a heavy-use item like a salad bowl because the varnish is a film finish (I'm a pretty dedicated "walnut oil" user for such things) but for hollowforms, decorative bowls, candlesticks and the like...perfect.

Re: Russ' finish

#8

Re: Russ' finish

Lynn Taylor

What method do you use to keep varnish air free?

Re: Russ' finish

#9

Re: Russ' finish

Bill Neddow

Lynn, I mix a quart of each of the liquids together well and then store them in the collapsible plastic bottles that Lee Valley sells. That keep the air out and they last for many months that way. I think mixing the other liquids with the varnish inhibits -- but does not stop- the tendency for the varnish to thicken.

Re: Russ' finish

#10

Bob Moffett

Re: Russ' finish

Bob Moffett

Thanks for the help everybody. I was guessing on the Mineral Oil.

Re: Russ' finish

#11

Re: Russ' finish

Lynn Taylor

Thanks for the info. Lynn