Wow -- the scale of that order is hard for me to grasp. Thanks for the real-world example. I may have to learn a little chemistry -- I'm just using Lowe's and Home Depot varieties of denatured alcohol, and I don't know how they compare. Incidentally, I don't really touch the stuff -- I have some tongs I use. I have three gallons in a five-gallon bucket -- and I'll have to look into how to know what the alcohol content is as I dilute it through time with displaced bowl-water. I'm just wrapping the outsides and rims of the bowls with paper and letting them sit around in the garage for a while -- but then, I'm not on a timeline.
Why waste time with the marginal wood-it doesn't matter whether or not you produce high volume, or just a few pieces. The amount of effort put into trying to work with crappy material is large....... Use the good straight-grained ( not to be confused with figured) wood. If you are getting cracks while you work it, all you need to do is keep the surface damp as you work. It really is that simple.
There's an article on my website that may, or may not, be helpful. My point is, many of us manage quite well without any of these problems, or "solutions", and what we do will work for anyone. Basic knowledge and a little practice and observation is really all one needs.
To Don Thur, you referred to methyl hydrate. I hope that you do NOT mean methanol, which is highly toxic. Generally what turners are using is Denatured Alcohol (DNA), which could be called ethyl hydrate. In its unadulterated form, as vodka, etc. it is OK to drink, for some of us. However, the denatured part adds some toxin to make it undrinkable (and untaxable) and therefore not good for you, either to drink, get on your skin, or breathe a lot of.
I have found that an overnight soak, followed by bagging, yields stable weight in 4-6 weeks.
John, thanks for the advice on the stock itself -- certainly cannot argue against turning better wood. And I'll be sure to look at your site to learn more about your methods. On the plus side for me, I also have my alcohol ready when necessary for helping with my reactive found wood. :-)
I think you are right about how the ethanol process works. I've dabbled with it now and again, but generally I rough turn pretty quickly, wet the wood with more water if its starting to dry while you're working it, and after a quick towel-dry, a coat of Anchorseal will slow down the drying as well as anything.
In truth, I now only use Anchorseal with pretty high-value wood, or pieces that I really can't afford to lose (like a commission to make something from Uncle Chester's favorite Elm tree, etc...). Usually, I rough turn and toss 'em in a cardboard box with no coating at all -- sometimes a paper shopping bag (no shavings, that's just a moldy mess waiting to happen). I never store drying wood in a heated space until it has air dried for a few months, especially if heated with a with forced air furnace. I lose very few pieces that way. I may only be lucky because where I live is quite humid during spring and summer, real nice in the fall, and pieces freeze solid in the winter.
I have turned a bunch of red and white oak in the past. Kitchen cabinets are typically oak in this area and a nice oak bowl on the kitchen table is appealing. That said, I have gotten some AWESOME CRACKS trying to dry oak. Oak has a very high shrinkage which leads to this cracking. The only solution I found for larger oak bowls (over 12") was to boil the roughouts for an hour or so. I then let them cool in the water and removed them. Left them out to air dry the surface and then bagged them. This method was made popular by Steve Russell and is in the archives or on his website. I only do this for Oak. Almost all my other bowls dry fine with a paper bag.