Re: Couple questions
Pascal Oudet
>Hello,
this big rasp is used for polyurethane shaping (1400mm long=55" * 120mm diameter=5", more than 100.000 hammer strokes).
after the rasp is stitched, yes it is heat treated (carbon steel XC48, I believe quenched in salted water, under controlled conditions of course).
regarding the rotating rasps (2" diameter), I'll have some new prototypes with me in Albuquerque, that I'll probably use in my "spiky creature" demo.
I must say I have no business affiliation with this maker, but he is a very nice guy, interested in how we use the tools and very open to inputs from users; we have been discussing needs and use of hand stitched rasps for some time, and he is developping new shapes based on this.
he's been doing this for 11 years, and the other guy we see in the video for 19 years. I was told 2 years are needed to get the skills, and only 12 people in France today still have the know-how. I'm happy if I can help them coming up with new products and continue this tradition.
Pascal