Re: Pewter inlay question

#26

Re: Don, Good idea!! Have you ...

don lewonczyk

>Ed, to be honest I haven't tried it on wood but the picture I saw with some of it in a turned bowl looked pretty good. I would think that if it sands out to a feather edge like in auto body repair it would also do good in wood. I know it says to fill up cracks in layers letting each layer dry good before adding more and it's supose to stick good. Anyway way if I get a chance I'll put some in a defect on a piece of seasoned walnut and maybe some on softer wood to see how it sands out. DonL

Re: Pewter inlay question

#27

Re: Pewter inlay question

Pascal Oudet

>Ed, I understand your concern about lead. just in case you havne't given up 100% on the idea:

the interesting characteristics in the alloy Christophe uses is the transition from solid to liquid: there is a pasty intermediate state.

without entering too much in metallurgical details, this can be seen on the phase diagram of this alloy.

I know Christophe has investigated with other types of alloy (I believe with some silver), I seem to remeber it worked at higher temperature. if you can find a lead-free alloy, with the same phase transition characteristics, it would work also. since Christophe is on your side of the Atlantic these days, maybe someone can ask this directly to him

Pascal

Re: Pewter inlay question

#28

Re: Pewter inlay question

Ed Moore

>Thanks, Pascal. I am reconsidering my options. I definitely want to use a "silver" metal in some form for the inlay. There is a liquid named "Lab Metal" that may yield the easiest solution.

Thanks for your help.

Ed

Re: Pewter inlay question

#29

Re: Phases

Mark Mandell - Gone Round In Jersey

>To simplify things a bit for those interested.

Lead melts at about 650F, Tin melts at about 450F. As a lead/tin alloy cools from being a full liquid, the lead begins to crystalize while the tin stays liquid until the whole glob drops below 450F. What you get is crystals (bits) of solid lead floating in a tin soup, with the consistency of mashed potatoes, that gets thicker as it cools. Since the difference in melting points is almost 200 degrees, there is a fairly long period of the "paste" or mashed potato consistency. This property was used by plumbers for many years to literally build pipe out of a lead alloy in place, usually to make the last connection between cast iron pipe and a toilet flange under the bathroom floor. With Ferncos, plastic pipe, and technology, "wiping a lead bend" is mostly a lost art. Good riddence as well, as lead fumes were always part of the process of using this very toxic metal.