Re: Just to stay accurate...
david weaver
This is an ideal steel for the smoothing you're talking about.
You're twice the man that I am if you could do jack work for an hour, sharpen and then continue on. I think I could do that once.
In the middle of this test, as this iron dusted my beloved shop made iron by a mile, I start to think "what I am doing making my own stuff?", but I cannot deny the sweetness of steels that work on the stones that I have the way I like.
I'm inclined to do a comparo test between O1 and an old ward blade. if the ward blade beats O1 by any significant amount, I'd be very surprised, but the older ward are water hardening steel and they are the sweetest thing in the world on oilstones.
You mentioned changing planes, maybe I responded to it already, but I made my own jack, and my metal jointer is a dandy I. Sorby jointer (which usually gets fairly little use in favor of faster working with the try plane - the metal plane gets used to finish edges/match joints and to work small things - occasionally if I'm working on something and the try plane isn't sharp, I'll use it out of laziness). The sorby jointer has one of the softest irons I've seen on a metal plane, but I will try everything these days. It would probably do horribly in this test, but drag it across a stone, it rolls up a wire edge, remove it and you're off again.
That is a draw for me to the shop. What would it last vs. the V11 - a third? I don't know. It's very uncommon for me to take 500 feet of shavings with it all at once. The inclusion that stopped the other test would damage it, too, but how long would it take to repair? three minutes, maybe.
I didn't set out to make this test something that would change my gear, though it's probably gone so far as convincing me to keep the V11 iron rather than sell it on ebay. I did think we'd be able to find 3V superior, and that V11 would be close to A2. In both runs (up to the point where the maple test stopped), I wasn't able to prove that. I suspect the record plane was a slight disadvantage for 3V. Was it 50 shavings? I don't know - it's not available on the open market as a commercial product, so it's not material to the test.
I'm over the moon with how the chinese iron performed, and I was actually using that one at the time of this test in a stanley smoother. There are some things about it that make it less ideal for a beginner, though (occasional voids in the steel, not flat when you get it and harder to flatten than A2 - the cap iron slides on the polished face of it - it's really slick and resistant to abrasives over a large flat surface).
If you're not sure about my thoughts that V11 would be brought back to earth, you can see the tirade I went on about LV's O1 not being as hard as I'd like, and wishing they would optimize those irons. Not that you need to. But, I was at the beach for the week and bored and supposing things before testing them. I just turned out not to be correct, and may have been a little bit out of line. When I ordered the V11 iron, it was on the heels of that, and I was a little bit concerned that my order might not get filled.
So, at least in the results of this test and based on the progress in the maple test, I was wrong. It happens.