How to get speed of application
Wiley Horne--So. Calif.
Hi Wilbur and all,
Wonderful work by your son, and wonderful you were there together!
I love hot hide, and have used it for dovetails, and for making one-off banding, like these (the first I ever made):

Still trying to get to the point.....which is how to get speed of application. These bands were made from scratch by cutting all the components with gouges; then picking up each piece to be applied with hemostats and plunging it into the hot hide; bring it out dripping and press it into place; hold it for 30 seconds to 1 minute; wipe hands on wet towel and go on to the next piece, and so on down the strand.
Similarly, with drawer dovetails, particularly smallish drawers, I can just plunge the two mating parts into the glue, then run them together with a mallet rap--done, and onto the next joint. It's very fast and sure.
Coming up soon will be a writing desk top, to be veneered with 1/8" strips, laid down on Baltic birch. For example, the center field of the desktop will be made of three 5-inch wide strips, 34" long; joined and glued down. (There will be more 1/8" thick crossbanding around this center field.) My thinking is to edge-join those three strips first, then glue the whole panel, 15" x 34", to the substrate in one go.
But whether it's done strip by strip, or all in one go, I have the same problem with hot hide: How do I get three surfaces covered quickly--the Baltic birch substrate, and both sides of the sawn veneer to be laid down? Am afraid of taking too long and getting a cold join. My thinking now is to use Old Brown Glue or PVA, each of which would require the same approach of covering three surfaces, but the Old Brown or PVA allow enough working time to get it all done without hysterics.
Incidentally, Patrick Edwards suggests a fine paint roller for the Old Brown Glue spreading, while Konrad Sauer suggested something he picked up from Michael Fortune--using a fine notched trowel (for thin set) to spread either Old Brown Glue or PVA. I think I'll use the trowel approach.
Anyway, to get back to the point--what do you folks do to speed up the process of getting the hot hide down onto multiple surfaces, in time not to end up with a cold join?
Thanks,
Wiley