Re: liquid hide vrs. hot
TomD
Truth!
The cold glue is modified with urea, or something to give it open time. There is probably other stuff in there. The end result is cheese spread. But you see it a lot of factories. As I keep saying, they almost always heat the wood. But that doesn't change the chemistry. Understand, the loads on guitars are crazy. But also on some furniture. Maybe stools. It is always hard to know what to do when you become aware of a better method, but it becomes necessary to leave a proven one to adopt it, only to find there was bear trap somewhere in the process.
Titebond old formula is also really good. Other stuff may be as good, but nobody wants to build one hundred guitars and get them all back in the mail under warranty. Or worse, put someone's eye out if a bridge snapped. LMII makes a better white glue, and I would prefer it, but it combines poor shelf life with huge expense to get up to Canada.