I think you might still find it in car clear coats, and boat finishes. Whether it would stick to your wood is another question, but it probably does. Easy to test. A lot of things do. Isos can kill you on the spot, but the glue on wet skin warning was more a cancer over longer term exposure risk, and one can simply work clean and with gloves. The paint inhalation dangers require positive pressure systems. Good results can be rolled and tipped which makes it possible to operate in an areas with abundant fresh air.
I recently had surgery and they glued me back together. I thought I was terribly bruised until I realized the glue was purple, sort of like the plumber's glue for PVC. The glue eventually pealed off with very little scarring. I have never figured out how a wound can heal if the edges of the skin are coated with glue.
The glue used to piece you back together is a variant of the cyanoacrylate we use to glue wood. However, it is slightly different to make it less toxic to body parts. Inside the wound it degrades rapidly, a factor that should cause pause when contemplating a "permanent" assembly of wood. I suppose one heals together as the glue degrades.
turns out daughter, the polymer chemist, is working with urethanes. The uncured glue has isocyanate parts on the polymer molecules which are wickedly reactive but won't react with themselves. When a water molecule finds an isocyanate part it turns it into an amine. A byproduct is carbon dioxide which is why the curing glue foams. If some other isocyanate then finds this amine there is a reaction that joins these parts together(cross links the urethane molecules).
Think of a plate of Spaghetti (urethane polymer molecules) and when water is added the Spaghetti strands become stuck together here and there at points along their length. The result is one mass of stuck together Spaghetti strands(urethane molecules).
The obvious conclusion is that if too much water is added most of the isocyanate will become amine and there won't be any isocyanate left to react with these amines. Foaming in the glue line will weaken the glue (air is a poor adhesive).
Translating to English, too much water in the joint will result in insufficient crosslinking to yield a tough cured glue. Foamed glue is not what one wants either. Other than slower cure I don't see any obvious disadvantage for not adding water. The possible advantage of not adding water is a tougher cured glue.
Gorilla Glue is 2 miles from me so I drove over and spent about 15 minutes with one of the customer support people.
As Bill said, water is needed to complete a chemical reaction. Uniform light moisture across entire surface to be glued is ideal. There may be enough moisture in two pieces of wood being glued together, but will take time for the moisture to migrate from the wood to the glue, so need to clamp for a longer period of time. No way to know how long, unless several similar sample pieces that can be tested one at a time several hours apart. Don't need a lot of water, because glue layer should be very thin. Also, she wasn't sure there was likelihood of surface of glue curing and keeping water from reaching interior of the glue line, because the glue line should be very thin. (this was a question mentioned in an earlier post)
Open or working time for brown Gorilla Glue is 10-15 minutes. Earlier posts identified carbon dioxide off gassing as the reason for the foam. Customer service suggested if surface of the polyurethane glue begins foaming before clamping pressure applied, within the 10-15 minute open time the clamping pressure will force the carbon dioxide out of the foam and the glue line will be as strong as if foaming had not begun.
Curing rate not affected by temperature within normal temp ranges.
Can thin brown Gorilla Glue up to 5% with xylene, then inject with a syringe. She didn't know how large the needle bore had to be.
There is a "white" Gorilla Glue polyurethane with an open or working time about half that of the brown version.
I need to try to affix bubbles in veneer glued with urea formaldehyde. I had pointed out to the customer that the old tabletop was not flat enough to reveneer and he said to veneer it anyway, wasn't going to make a new top. So there is distinct possibility the bubbles that formed are over the low areas, and that the veneer wasn't pressed down into the urea formaldehyde glue by the vacuum bag and caul. I had spread a slightly thicker than normal layer of glue, and placed layer of heavy canvas between veneer and caul hoping it would compress enough to push veneer into the glue at the low spots.
I will try Gorilla Glue poly either thinned with xylene and injected with a syringe, then in vacuum bag for 24 hours; or by slitting the veneer, lightly misting some water into the slits, waiting 20-30 minutes for the water to be absorbed into the veneer, working some unthinned poly into the slits, and then into the vacuum bag for several hours. In either case, it may still not work if the areas of the tabletop under the bubbles is still low. I plan to look for some compressible cork I can use to try to push the veneer down enough so the poly doesn't have room to foam.
I think this summarizes all I learned from the Gorilla Glue customer service rep this afternoon.
Don, you added some additional information on what you're planning to do with the poly and I would suggest using superglue instead of poly for your repair work. Slit the bobbles along the grain with a scalpel and inject a small amount of superglue into the slit. Cover the area with a piece of plastic and work the glue around with your finger to spread it inside the bubble. The plastic keeps the glue off your finger. Use small cork covered cauls and clamp them in place until the glue sets; skip the vacuum bag. If you can't reach to the bubble with clamps lightly spray the glued area with accelerator and press the caul down with body weight for a minute or two. Make sure you keep teh plastic between the glue and the caul.
Had you used white or yellow glue you could have simply steamed the bubble which would have reactivated the glue, then mashed it flat with a clamp of some sort to stick it.
Back in the 80s Climbers were gluing chunks back down with hardware store crazy glue. I always wondered how they got the lumps out, but apparently not a problem. I was more a press and hold guy.
I was bored one night and started researching cyanoacrylate adhesive. Around the Vietnam war erra Eastman chemical (Kodak to us photographers) was exprimenting with long chain polymers. To make a long story short they developed super glue and found it was excellent to instantly glue human skin together. I oicture some guy with his fingers glued to a test tube flinging it around while his buddies laugh. Anyway they developed a sterile version and called it Eastman 310 adhesive. It was used in Vietnam to close wounds quite successfully.
The polymer was being investigated for various applications, for example aircraft canopies. Indeed its adhesive properties were discovered by accident when it glued some test equipment together and its inventor's arm to a lab bench. It was great fun to tick someone into putting a drop on their finger and then touching the other with the result that they were instantly stuck.
Eastman sold the glue as Eastman 910. It was investigate for all sorts of application, for example gluing horse shoes onto horses. It was a failure in the market place because its shelf life was unpredictable and it didn't make a permanent bond in some applications. The rights were sold to Locktite who figured out how to make it more stable. This is the same material we know know as "super glue, etc.".
When researching its degradation over time I found the person in the Army that made it for wound closure, presumably under license from Eastman. It was well known at Eastman that it was being used for wound closure but it is unclear to me if material made at Eastman was used or whether only the material made by the Army was used. A slight variation of the glue made it less hostile to tissue. It is rapidly degraded by moisture and the body breaks it down and eliminates it in the urine in a matter of days, a factor to consider when gluing moisture containing wood together. This is the same glue used today for wound closure.
If they were "nice" we would tell the person with glued fingers to just hold them under water for a bit and all would be well. Others used razor blades.
I use white Gorilla to glue brass tubes into wood and acrylic blanks. I let them cure overnight. I don't moisten wood but for acrylic blanks I take a big breath and exhale through the hole. That is more than enough moisture to cure the glue.
First, I went to the emergency room a couple of years ago and had my lower lip glued back together after a silly home injury. I askd the doc about using super glue in the shop in the event of a serious cut. She told me that the variety of cyanoacrylate they use is designed for medical use, but that, in a pinch, the shop variety would do. She told me it apply it in strips across the skin, pependicular to the cut to hold the separated tissue together like a piece of tape, and definitely not to apply the glue to the inside of the wound.
Second, a while back I was attempting to glue some small parts together with cyanoacrylate glue while holding them together with my left hand. The spout on the glue bottle clogged, so I squeezed the bottle pretty hard to unclog it. Well, that was a mistake. The top popped completely off the bottle and flooded my hand with glue, bonding it instantly to my bench top and the parts I was attempting to glue together. For a moment, I had visions of great pieces of flesh stuck to my bench top after I extricated my hand. Fortunately, I had placed the bottle of debonder within easy reach. I spied it and flooded my stuck hand with it. Slowly I was able to free my hand with no loss of skin or flesh. I felt pretty stupid, but thankful I was uninjured. It's amazing how quickly something so simple can turn into a potential disaster.
From what I have read the stuff we normally buy is hostile to raw flesh, killing the cells it touches. Increasing the molecular weight of the ester part of the molecule makes the adhesive more benign. I have read that the butyl ester is used for medical application.
A huge amount of heat is released when the glue polymerizes(cures). If you spill a lot on pants, for example, a burn could result, to say nothing about your pants.
If all ease fails flood the area with water. The cured adhesive degrades in water and will eventually let go.
The heat release was very apparent when I glued my hand to the bench. I thought I would have blisters, but I was lucky. I did have some areas where I had superficial skin loss, but I didn't notice any large scale tissue destruction.
To add to your narrative, the U.S. Army Biomedical Research & Development Laboratory (located first at Walter Reed, then Ft. Detrick) was the facility that prepared the cyanoacrylate adhesive for the Vietnam solders and conducted research on the degradation properties of various adhesive analogues. While all cyanoacrylate adhesives degrade by the same mechanism (reverse Knoevenagle), the butyl analogue was chosen as the adhesive to synthesize and send to the Army medics. It degrades more slowly than the methylcyanoacrylate, hence the soft tissue is able to handle the decrease in pH and production of formaldehyde that is produced when the adhesive degrades. Stability was an issue, but that problem was largely solved. Because of the tissue irritation issue with some of the alkylcyanoacrylates, more benign (yet still rapidly degrading) analogues were prepared by an entirely different synthetic route.
Unfortunately, with the Vietnam war winding down, the Army closed down the portion of the lab devoted to adhesive development (and many other medical products - degradable sutures, blood-clotting bandages, bone cements etc.). The lab was, at the time, unique in its capability. From synthesis of medical polymers, including radio-labeled, to implantation in animals, and histological evaluation - all on one floor. As a polymer chemist, it was one of the best jobs I ever had. Thanks for refreshing those memories Bill.
As an interesting side note, Bill Cosby's father-in-law (Guy Hanks) was the technician who made many of the adhesives for the Army. Anyway, sorry for the long digression. Jim
I could not remember who I corresponded with some years ago on degradation. I have saved your additional information as well as sent it on the some Eastman people who will be interested.
I haven't had much trouble using medium thick CA glue. Much faster. Once in a while, if the hole isn't quite right, the tube does get stuck half way through. Bummer! The thing is, I really don't want to wait long to get going on the lathe.