I'm working on a column base,
Keith Newton
For one of the older homes a few blocks up my street. The columns are 12" diameter at the bottom, and my turned base will be about 5.25" Tall, and about 17.5" D at the bottom layer.
I'm gluing up 3 layers, with 6 sides mitered in each level, that will be glued together like a layered cake.
Everybody knows that a frame with mitered corners will self destruct if there are swings in the MC of the wood, and the wider the boards, the more extreme it will be. If the wood gains moisture, the swelling across the grain will open the toe, or outside corners of the miter, then if it goes below the starting point, the heel of the miter will open. I plan to really soak them inside and out with CEPS after turning, to help stabilize them, i hope.
When I glue the 3 layers together, I will be brick-laying, or staggering the joints, so the joints don't all line up in each layer. I was just pondering this, and wondering if it is better to only shift the joints about and inch from each other, or brake the joints about midway in the length of the next layer.
I'm inclined to think less it will be better for the glue joints between layers, if the joints are only slightly offset. This will keep the grain alignment closer between the layers, which will cut down on the shearing effect on the glueline, if or when the wood moves, than shifting the miters half the length of it's neighbor.
I don't recall ever reading anything where this was discussed before, and would be interested what others do, if I have missed catching it as I was learning my craft. What say ye?