Re: The real story, and o-rings
TomD
Nobody could be a more fervent WEST supporter than I am, but these days there are a lot of products to choose from. Actually, my 5 minute is also made by them. On YOUTUBE, you can see a video where they repair a carbon spar using West 105 and 5 minute to speed up the cure. Their 5 is pretty good, as is Devcon. The main reason to use WEST it it's superior structural properties.
If you want to colour the 5 use something that isn't a thixotropic agent also. Sawdust is also a little too large, and does not compact well, so in small repairs it often lacks correct granularity. For repair I normally mix in whatever will blend best. So I might use carbon powder if I was trying to ape the black pigments in cherry.
For outright hiding, super glue is usually the best approach, but you can't be filling too much. With super glue and sawdust one can make invisible repairs, with epoxy even if the dust starts out the same colour it normally ends up a lot darker.
For dispensing small amounts of epoxy, I use o ring syringes. I haven't used this place, but it looks good:
http://www.squirrelsandmore.com/rehab-supplies/oring-syringes.html
These will hang in there indefinetly, and they do not pop off like some of the rubber plungers. For really long term use one could substitute epoxy compatible O-rings.
With the 5cc syringes I use, the trick is to drill a 3mm hole in whatever cap comes with whatever you want to dispense, and then mount the syringe in that hole, it will be a an air tight seal. Once, before we could buy all this stuff online, I scored 25 of these syringes at a very cheap price. Up till then they were 3 dollars each in drug stores. Anyway, with the windfall of syringes, I mounted these babies in virtually every bottle in the house, from detergent, to epoxy.
For larger projects I am supposed to be making a machined aluminum pump, but my laziness knows no bounds.