Home Articles Forums Gallery Marketplace Videos

WoodCentral Forums

Knowledge You Can Build On — Est. 1998

Build it. Rock it. Rockler has your woodworking tools.

Finishing

Posts

Finishing

#1

Finishing

Jack Hartley

Hi everyone!!

I am building a Mission Style blanket chest out of quarter sawn white oak for my oldest daughter�s college graduation. When I build different projects I try to learn something new each time. This time it is using TransTint dye for the first time instead of the premixed stains.

I have read that you can use water, alcohol, and many other solvents to apply the tint. Of course water will raise the grain; alcohol I have read requires spraying because of the evaporation rate is too quick for brushing or wiping. What solvent should I use apply the tint?

The top finish is going to be Waterlox, can I mix the tint in the first coat of finish and then apply the additional coats of finish with out the tint? Do you have to apply the tint coat using some other type of solvent?

What are the mixing portions of tint to solvent?

Thanks for your comments

Re: Finishing

#2

Clint Searl

Re: Finishing

Clint Searl

Unless you're spraying the top finish, use a dye stain that is soluble only in water, otherwise the the finish will pull it. If you're going to brush on a waterborne top finish, I would go with an oil based pigmented stain.

Clint

Re: Finishing

#3

Re: Finishing

roger lance

Jack....do a search on Jeff Jewitt for his finishing schedule on QSWO....he's the maker of TransTint....remember, do not use an oil based product as final coat for inside of chest...that could also be coated with de-waxed shellac (alcohol based).

Re: Finishing

#4

worth a try

Jesse Cloud

Try tinting a little of your waterlox directly with the Transtint. Rub on or brush. Try it on some scrap of the same wood. If you like the results, it will save a lot of time and trouble.

Re: Finishing

#5

Clint Searl

Good idea

Clint Searl

Re: Finishing

#6

Re: Finishing

Todd Nebel

Hi Jack,

I sand QSWO to 220 and wet it pretty heavily. After it dries I sand it again with 220. I apply a waterbased dye with a cotton cloth and blend the color evenly. After it dries I would put a thick coat of waterlox and keep applying it until it stops obsorbing. Then with a wet dry 500 piece of sandpaper I work it in some more and cut down some of the raised fibers. Then wipe off the extra and let dry. Then lightly sand and light coats of waterlox. After a month I go back and cut down the sheen with 0000 steelwool and wax.

Todd

Re: Finishing

#7

Won't Work

David Yoho

Trans Tint dyes do not dissolve in oil based finishes like Waterlox unless an additive available from Homestead Finishing is used.

Re: Finishing

#8

Clint Searl

Huh?

Clint Searl

From the Homestead website: One of TransTint Dyes most unique features is their compatibility with a wide range of finishing mediums. Simply add the dye concentrate directly to shellac, water-base finishes, solvent lacquers, and catalyzed varnish or lacquers. Add any amount up to 1 oz. per quart. All 19 dye colors (10 wood tones & 9 accent colors) are intermixable to produce custom shades.

I have used it to tint solvent lacquer. So why wouldn't it work with Waterlox if pre-disolved in any compatible solvent?

Re: Finishing

#9

Re: Huh? *LINK*

David Yoho

I've tried it once and it didn't work. But to refer to Homestead's own information, here's what they said in a PDF document linked below -

� TransTints are not recommended for adding to oil based finishes like stains, varnishes, polyurethanes, linseed and Tung oil. You can usually work around having to add TransTint to oils by using TransTints in shellac or some other medium that it does mix with. If you have a situation where you must add TransTints to any oil or oil product that thins with mineral spirits, contact us for an additive that will disperse the dye into oil finishes.


Trans Tint PDF

Re: Finishing

#10

Re: Finishing

Steve Schoene

Clint's suggestion about the powdered water soluble dye is a good one. TransFast is Jeff Jewitt's version.

With any dye, you may find that the inside of the pores doesn't "take". If so you may need to use a pigmented oil stain over the dye. Sealing the dye with shellac before the stain prevents the stain from having too large an impact on the color. The combination of pigment stain over dye is a good one and adds depth to the finish. You can make your own stain. Mix the waterlox with a little BLO to slow it's drying time, and add artist's oil paint for pigments. (Or japan colors or UTCs) I shoot for a stain color just a hair darker than the dye to let the pores pattern standout but only a little, not nearly as much as a stain only coloration.

To mix dye you have to make tests on the same wood as your project. Note that when dye dries in can look awful until a topcoat (or a simulated topcoat like mineral spirits) is applied over it. So don't judge either the color or the intensity until you have added the top coat in your tests.

Re: Finishing

#11

Re: Finishing

Todd Nebel

To combat the "inside of the pores doesn't take" effect of using a powdered dye desolved in water, I apply a gel stain and work it into the pores. Then finish with a wipe-on varnish.

Re: Finishing

#12

Add acetone to your tint...

John in NM

I've been able to use transtint in tung oil by mixing the tint in a little acetone, then adding it to the oil. Usually I'll do this with a first coat using tung oil from Woodcraft, then top coat with Waterlox. You can probably tint the Waterlox directly, but it may not be as simple as tinting tung oil.

If nothing else, the Original Sealer/Finish Waterlox is dark enough that it would be hard to tell if you have a good mix or just little globules of tint in the bottom of the mix - with tung its easy to tell. Some of the other Waterlox products I've used are lighter and might be easy enough to distinguish the tint from the oil if they don't mix nicely.

I can't help with the proportions, I've been doing small amounts in a "little of this, little of that" sort of fashion.

Re: Finishing

#13

Clint Searl

Very interesting

Clint Searl

The omission of that tidbit from their product blurb seems deceptive, leading to potential problems.

Clint

Re: Finishing

#14

The only downside I've found...

John in NM

With the method I mention below, is that it tends to make the tung oil gel after a few days. Adding more turpentine seems to slow the gelling.