I mixed up some System Three T88 one hour epoxy and added a bit of color. A tiny amount of powdered dye to match it to the walnut. I thought I got the mix right and if anything a little heavy on the hardener. After four hours the exposed part of the epoxy is gummy. Is there any chance this is going to work? It's in some through dovetails I thought were a bit loose.
since I used that brand, but, I would caution against changing the mix. You may think adding more catalyst would make it harder, but it may actually have opposite the effect, not to mention adding the dye.
I like to stick with the mix ratio, then add color by adding wood dust from my sander bag to thicken and match color.
If you didn't get the technical manual for that epoxy, you ought to get a copy and read it.
Epoxy is like making coffee. It only requires that you mix two things. Anybody can do that, but there are lots of tricks to may lead to success or failure if you fail to follow ALL the rules.
System Three suggests that in quantities less than a cup, that you mix by weight rather than by volume.
You need to adhere to the exact ratio for your product. If you use epoxy paste colorant, its counts as resin,; pigment or dye, however, is not counted because it will not react as resin. When you tried to compensate by adding extra hardener, you messed the chemistry. It will most likely get to a semi hard state, but no further. Suggest you dig it out and try again. Mix your resin and hardener precisely, then add the colorant. For wood joints, I like to use wood flour as it colors to match and also makes the mix thixotropic (sp) so it stays put in the joint.
The chemical reaction between the two components is temperature dependent - if very cold, it takes longer time.
Epoxy has a limited shelf life, particularly the "hardener" part absorbs moisture from the air and deteriorates in a year or so.
Not adhering to the correct mix ratio will leave the excess component without something to react with and leave a gummy result.
Thorughly mixing is required. If not proprly mixed, the two components cannot get together and react. Mixing small amounts is often difficult and getting the proportions right in small batches also makes ratio errors larger.
If it does not harden properly in room temperature in a day or so, you are SOL.
used a little set of spring loaded postal scales and this was a small batch. The reason I thought I might be "long" on hardener is that when I started the two components seemed to have identical amounts in the bottles but after several hours of sitting on the counter the hardener seemed a little low, thus a little extra went into the batch.
I had a set of electronic scales for this but they went the way of the Buffalo. I need to ask my son where they went, but he has lost his cell phone. I don't want to think about what he is weighing. (Actually, it is probably snakes, he raises exotic snakes.)
I did not know there was a shelf life. I thought in a previous thread someone said it would last a very long time. This is over a year old.
I need to find a reliable way to mix small batches. It seems that's all I use.
I had varying results with Sys-3 until I bought a little electronic scale that weighs to .001 gram + has a tare function [Amazon - $15], and I e-mailed Sys-3 support and asked for the exact mix ratio by weight. I use System Three General Purpose resin + fast hardener and the ratio is 100 > 44 (with epoxy paste colorant as part of the 100). Using that ratio I've had "perfect" results every time since on the stuff, even down to the 1/10th oz batches I use to fill turning's holes.
BTW, my 1 quart "kit" of resin and hardener is well over 4 years old and works just fine when properly mixed.
I used to use a of an epoxy that is very similar to system three, it even has three different catalysts to shse from. I bought all my supplies from Tap Plastics, a Ca companie that makes and sells their own brand of resins and supplies.
The one item I used to get from them that I have not found anywhere else are some little cups marked in mili litere, oz. and drams. there are made by sweetheart and are the size of the smallest dixie cups. I used thes for mixin as little as a table spoon and never had any problems.
One thing that I alwyas did when mixing small amounts was to mix extremely well, making sure to scrape the sides and bottom. Then pour into a clean cup, and this is the critical part, you only pour it into the clean cup and DO NOT SCRAPE THE SIDES. Then mix it in the clean cup using a fresh stir stick. This may sound wastful but it is a trick I learned when I was making molds for a living. there is nothing more wastfull than making a mold and having a batch in the middle fail to go off properly or to have a sterak of goo in the middle which becomes a soft spot. in a production setting you use the second container as the first container for the next batch so it really only requires one additional comntainer to make an entire mold tis way.
The other thing I always do is write down the mix ration and the amounts for the batch I will be using and or I also mark on the sides of the mix container with a sharpie, this may sound remidial but it has kept me from making stupid mistakes.
I get mine free on take-outs for mustard and duck sauce from the Chinese joint and for salad dressing from Luigi's. They're polyethylene "Solo" brand, and are the perfect sizes to make small batches, plus, before the mix sets up, they wipe clean for reuse with a bit of DNA and part of a paper towel.
It was slow, but it did set and was hard to the point of being nearly brittle. Maybe the shop temp was a little low and slowed it down, but by morning it was good to go.
I still need to improve my ability to make small batches.