>I`m making the picture frame in the picture down below, if it posts. It`s being made out of red oak and it`s very wide grain, like most evrything is nowadays. How would a person go about finishing it off to get a smooth finish. TIA Larry in Ohio
>The only way I know to get red oak really smooth during finishing is to use a pore filler. The open pores of red oak are like canyons compared to many other woods. They'll need to be filled to give the same feel as the wood used in that photo.
>I use nothing but Red Oak for bases to mount my work on. Its cost effective ( for me ), forgiving, and extremely stable when finnished. I start with rough then fine sanding and then start with min-Wax polyurathane ( satin or gloss ) five or six coats ( just 'till the stuff " takes " and fills the pores and grain ), sand fine. Then another five or six coats normally does the job. Might need another REALLY fine sanding with another four or five coats. The finnish is glassy smooth with a glassy gloss finnish OR satin and can be dusted or cleaned without worry. It'll also out live pretty much anyone.