Shellac Finishing

#1

Shellac Finishing

Gary Poduska

>I am trying to get a mirror finish on my pens that I turn. I have been sealing with CA (superglue), sand down and finish with glossy urethane. It works great, but after a frew months, the urethane tends to peel in spots. Im not sure if i need to rough up the CA a bit prior to applying the urethane.

My question is, will using shellac flakes on the lathe to seal (8lb cut) and then a 4lb cut repeatedly will gve me a mirror finish (like a french plolish). since pens are very small, Im thinking i can give them a french polish fairly easily. will this work?

Re: Shellac Finishing

#2

Re: Try posting on the Turning messageboard

Larry Clinton At Frankfort (Central)., Indiana

>Although some may answer here - there is a lot of expertise on that board & I'm sure they can help you. Just click on Turning under the MESSAGEBOARDS column on the left.

Re: Shellac Finishing

#3

Have you tried?....

David Yoho

>Have you tried Zinsser's French Polish? Woodcraft carries it, if you can't find it.

David

Re: Shellac Finishing

#4

I use it

bill tindal, E.TN

>It is easy to get a mirror shellac finish on the lathe. But it doesn't seem to me to be a very durable finish for a pen. I use it on ornaments. Just put it on with a hair brush, about 3 lb cut. Very slow lathe speed and let the object turn against the brush heavily loaded with shellac

Why are you using CA under urethane. It is picky about what it sticks to. Why don't you just use the urethane?

Re: Shellac Finishing

#5

Re: Shellac Finishing

Fog Tanner

>I am from the turning side, and I do some pens. I use a friction polish on some of them, which is shellac. I have also used some shellac I have mixed up myself. Typically this is a 2 lb cut, brushed on. The other is wiped on with a paper towel. Using a Viva paper towel, either one can be friction dried in a few seconds and repeated. I am generally spinning the pens in the 3000+ rpm range as you need the surface speed. Several layers can be built up fairly quickly.

I have also finished with just CA glue and nothing over it. You can sand CA down with 2000 grit wet or dry(wet - mineral spirts) and get a glass finish which will last longer than the Shellac. For the pens I am using shellac and no CA underneath, I will polish the wood further with EEE-Ultra shine, which is an abrasive (rotten stone) in wax. The Shellac has no problem going over this. I also use this on other spindle items where I am looking for a gloss finish.

However, most of my pens have a satin finish. The satin finish will not show the scratchs as much and when the finish wears off from use and is replaced by body oil it is not noticable. I also use Titanium gold for the same reason, when the gold wears the Titanium is exposed and is the same color as the gold.

I don't use any of the long curing time finishes on the lathe, but if I were going to I would use one of the finishing resin (thin epoxy). I have worked with these in the past doing model building and could wet sand (water) these to a glass smooth glossy surface. Takes several days for the epoxy to get hard enough to sand, but it will stand up just about anything. And it doesn't lift if applied properly. I am working on a "project" bowl that I have to use this finish - the wood is less than sound (i.e. pretty punky in places).

Re: Shellac Finishing

#6

Don't get hooked on it

Michael Dresdner

>Don't get hooked on Zinsser French Polish. It was a wonderful material, possibly the best thing that ever came along to let novices French polish first time out beautifully, but it was discontinued last November. Anything you find is remaining stock in stores and will not be replaced. I am still trying to get them to either come out with it from another division of the company, or let me offer the formula to a small manufacturer. So far, neither. They own the formula, so it is their right to produce it or not.