Re: Question for Andi and other jewelry makers/
AndiWolfe
>Barry - I prefer a 50:50 mix of Danish oil and mineral spirits.
I hand sand to 400 grit, then sand using 3M bristle brushes - up to 400 grit, then buff with a hair wheel (3/32 mandrel). I use a micromotor carving unit for the last two finishing steps I just mentioned. This finishing sequence puts a nice sheen on the wood, even without a finish. The oil/mineral oil mixture soaks in and gives a good finish without the high gloss.
For turnings, once you get the sanding done, I'd do a bit of buffing with a scotchbrite pad - the white one works well, and then use the 50:50 oil/mineral spirits finish. Apply the finish off the lathe - liberal coat, let it soak in, wipe off.
Post a pic - I'd like to see what you made. Andi