>John, I've ordered a piece of 3/16" drill rod. They say I'll have to temper it once I get it cut to length. I would like to temper it if I can, so it will be harder than my gouges... And I don't know how.
I want to use it as a hardened edge on my toolrests.
Is there a way I can do this at home, or do I need to find someone with a kiln?
Any answers you can give me will surely be appreciated.
>Allen Try cutting it first. It my not be that hard. Take the edge of a file and run across it. If the file just skips across then you won't be able to cut it with a hacksaw. If the file makes a cut then it will saw. Most drill rod I've gotten is hard but not hard enough to cut.
To make it harder than your tools is going to be tough to do at home. At least for anything longer than a few inches. You would need to heat the entire rod to critical temperature and then quench it. This isn't hard to do over a few inches but would require a pretty good torch or furnace to do a 6" or 12" rod.
How are you going to fasten it to the tool rest?. If you plan to weld or braze it to the tool rest then you will defeat the purpose of hardening it.
I think drill rod will be hard enough as is. Not harder than your tools but will be much harder to dent than a cast steel tool rest.
>Drill rod usually doesn't come hardened. Did you order O-1 drill rod? That is an oil hardened rod. It should cut with a regular hacksaw. To harden, heat the rod to cherry red and quench it in vegetable oil. After you harden it you can temper it in your oven. Heat it to 350 deg. Tempering makes it a little less hard and not as brittle I believe Alan Lacer gives the instructions on his website. It�s the process he teaches to make hook tools
>The way I did it was to create a tube to quench it in. I used a piece of four inch duct work and taped the seam and the bottom with aluminum tape to seal it. I taped it to a board so it would stand up securely. I had some ancient exterior stain (packrat gene pays off again) and I poured the oil out of the stain in the tube. The depth of the oil was deeper than the length of the rod.
I held the rod with a pair of pliers I don't like and heated the rod with two torches until it was red hot and held it there until a magnet would not stick to the rod. I then released the pliers and allowed the rod to plunge vertically into the oil. The quick plunge was to allow the rod to fall in without setting the oil on fire. It passed through the surface so quickly it did not heat the oil on top enough to ignite it. My son was operating one of the torches, we did this at dusk outdoors so we could see the red color better. I was skeptical about the magnet not sticking, but after a minute or so, it lost its attraction.
Now that I read this, I must have been obsessed. I bought "oil hardening" steel. Would have been much simpler to buy water hardening and just heat the rod and toss it into a bucket of water. Nah! My way was much more fun. The risk of a conflagration, justified saving the stain to reuse the oil, making a strange small container, Playing with TWO torches in the dark and a MAGNET. It was a father an son bonding moment. (Its good he recovered from the burns and is not at all resentful)
If your tool rest is cast iron, almost any steel will be harder. If it is cast iron, it is very difficult to weld cast iron without special welding rods and skill. Braze it instead.
Allen I assume you are going to epoxy the rod to your tool rest.
So make your rod red hot and dump in water, this is not going to be a cutting tool hanging off the end of holder, as it is supported over its whole length it will not break by having a tool pressing on it.
It will be hard and not have your lathe tools mark it up.
The hardest thing might be keeping it straight while you heat it up, holding it in a vertical position or have it supported is your best bet.
>Allen : Unles you enjoy the process of tinkering with strange stuff, just weld up a tool rest with two pieces of cold rolled steel and resign your self to getting out the file occasionally.
I'm no blacksmith or metalurgist (or spelling teacher!) but I have been taught that water hardening steel (I think A2 falls in this category) is MUCH more difficult to harden at home. I believe there is more to it than simply heating it and plunging into the water. There are other factors involved. From what I have been able to read and learn, I'll stick with O1 in my make-shift home forge.
>You are right, but I was trying to express what Leo said better down below. My idea was that the rod would be completely supported and did not need to be tough and strong, but straidght and hard. Might be bad metalurgy, but functional. OTOH, if you could find a prehardened rod the correct length, you could just glue it in place with epoxy.
The quest here is to find a rest that does not get damaged and does not damage the tools. Probably be better to "absorb" the damage on the rest than on the tools. Rather file the rest than repair the tools.
>This makes great turning tools but the 3/8" rod would do well for a toolrest edge. They used to have 1/4" in the 8" length, but no more. You don't have to mess around with hardening it yourself, so $4 should be worth the time saved.
It should last forever, I'd think. I have JB-Welded this stuff to an angle iron toolrest and it's slicker than anything.
Grind the edge of the toolrest flat, degrease everything with acetone, and use duct tape to contain the JB-Weld or epoxy while it cures.
>You can make tool rests from either steel angle shapes or wood with a piece of music wire held in place with JB weld along the top edge. Music wire is available in 36" lengths in 1/8", 5/32", and 3/16" diameters at hobby shopsor hobby dealers on the Internet. It is prehardened and you will have a hard time finding a piece of steel that is harder than music wire. You have to cut it with a Dremel cut-off wheel.
>I didn't explain myself clearly. I expect to use the drill rod along the length of my three Oneway Toolrests. One is 6", and the other two are 12" lengths. And I do expect to JB Weld it on, some info that I got from WC several months ago. I knew that regular welding would take the temper out of it.
Now. The drill rod is supposed to be quenched in Oil or Saltwater quenching type stuff. I don't even know what temper means unless they want me to make it mad. Kidding. I just know that tempering makes it hard. If it's already hard enough like it is, that would be great. I believe it's called O-1.
I just want something harder than the soft steel of my toolrests. I don't believe they are cast Iron. And I am shakier than an Aspen in the wind, and it's hard enough for me to get a smooth cut, as it is, and I'm tired of having to stop in the middle of a turning to smooth the top edge of my toolrest.
I wish I'd known about that "music wire" beforehand. I thought music wire was something like piano or guitar strings. :o) I'd like to get some of it in a 3/16" size. So I may go that route.
I've learned some things from your posts, and again, thanks to all of you for your input.
Just to clear some of this up for you. You quench the steel (O1, W1, ir whatever) in the specified medium to harden it. Temper is the process that removes a small amount of that hardness and gives you back a measure of toughness and removes some of the brittle. You do this at a much lower temperature.
Recap: harden by heating to critical temp (1500+ degrees) and quenching, then temper at 350 degrees (or whatever is appropriate) in the oven.
I was going to include a link to a knifemaking site that has a great and very understandable treatise on heat treatment, but I find I now have so many links saved I cannot find the ones I want.
>I'm so offended I'll never answer one of your posts again! NOT REALLY! I want to clear up something for you though. Heating and quenching harden the steel. Tempering actually is a controlled softening that takes the brittleness out of the steel and makes it tougher. Tempering takes place a lower temperatures and the steel is allowed to cool more slowly. Here is a link to the Wikipedia page on tempering which tell us more than most of us need to know. Have fun turning. I haven�t been able to turn for 8 or 10 weeks and really miss it.
Tom
I'm so offended I'll never answer one of your posts again! NOT REALLY! I want to clear up something for you though. Heating and quenching harden the steel. Tempering actually is a controlled softening that takes the brittleness out of the steel. Tempering takes place a lower temperatures and the steel is allowed to cool more slowly. Here is a link to the Wikipedia page on tempering which tell us more than most of us need to know. Have fun turning. I haven�t been able to turn for 8 or 10 weeks and really miss it.
>...drill rod to be plenty hard enough without any further processing. I have a rest made in this manner(welded to a steel base) and it seldom has any noticable surface nicks and I primarily use it for my boring system. I bought it years ago already made and believe the brand name was Wood River? Woodcraft also used to have a similar product but I haven't seen them in stores lately.
>Thanks, Bob and Jamie, that's what I was wanting to hear... that it's hard enough as it is. I think if I just cut it to length with my Dremel cutoff wheel, and then JB weld it along the edge of my toolrest, it will work fine. It will be supported along it's entire length, so it won't matter if it's a little brittle.
>Thanks, Ken, this is the place I ordered my drill rod from... Houston Store... and I would have ordered this HSS rod, but they didn't have it in the right length for me. I have to have two 12" pieces and one 6" piece, so I just settled for the 36" drill rod.
Appreciate the tip about the tape to contain the JB, too. :o)
>Howdy Allan: I recently used 1/4" O-1 drill rod on the top of 4 tool rests I purchased from James Johnson (Kerville, TX). I cut a groove in the top with my 3" cut-off grinder, and expoxied it in. It is more than hard enough as it comes without further hardening, tempering, etc. Try it the easy way - I think you'll be happy. - Ed
>Howdy Allen: I haven't tried 3/16" so I can't say for sure. I think a lot depends on what you want to do with it. For instance, I have a 1-1/8" round tool rest that works great for large work. But, the tool is always resting at least 9/16" away from the edge of the rest. For delicate work, that's a little too far. I'd say for delicate work, especially on a mini lathe the 3/16" would work just fine. James' tool rests are 1/4" thick so the 1/4" drill rod works just perfect for that.