>After reading the grinding thread below, I thought I would start a new thread to give a recommendation to this little tool. I don't know why the woodworking tool suppliers haven't picked these up and adding it to their line.
I have been using a Koolmist brand sprayer for maybe 20 years, then ran across this little cheap one not long ago, and gave it a try. This is a great addition to the standard bench grinders if you want to make sure not to overheat your tools.
I have nothing to do with this company, but I do like the product, and think a lot of you could benefit from adding one to your grinders.
>Those are pretty cool. :) I've use something similar in a machine shop but really don't want the mess in my shop. Of course if you use a wet wheel grinder you solve the problem.
>A product designed to spray water on my grinder not intended to be a wet grinder. I don't think so. Why bother when the steel we use are not affected by the normal temperatures we subject them to. Meaning HSS. It would be interesting to find some other uses for it. I use the flexible fitting system to direct a blast of air to synthetic pens blanks when drilling on the drill press. I find it helps keep the cooler and reduces blow-outs.
>... that for those that have a water coolant based grinder, or want to build one, this is an affordable addition.
But more importantly, for those of us with a basic dry grinder, the Air Coolant (which is controlled separately... meaning I don't have to use the water) can be used without the water and we get some benefit of additional cooling.
>Only I don't think this would harm any grinder. The small amount of mist directed right into the interface of tool and wheel has a tremendous cooling effect on the cutting edge.
First, The air being compressed going into the tank of the compressor raises the temperature going in, but has dissipated while in the tank. Then when it is released through a small nozzle causes a drop in temperature, but atomizing the liquid at the nozzle tip drops it even further, Then any moisture that hits metal over 212� will turn to steam, and take the heat away in the form of steam better than anything.
I t sounds like there are some skeptics that must be imagining a lot more fluid than is actually being used, and might do well to see this in action to appreciate what a cool alternative this is. I don't claim to be an expert on metal tempering and annealing. I usually assume that the tool maker provides the tool at its best level of hardness, and I try not to change that.
I have made quite a few of my tools, and to assume that grinding doesn't change the hardness might be a little misleading if you don't ever do anything to test the assumption. One little tool that I find to be very handy is to cut my old disposable hhs planer knives in half and use the ends as scrapers. I sharpen them just like I would a chisel, then with a burnisher roll a burr on various shaped ends. If I sharpen with the mist-unit, the metal it too hard, and will break before rolling over into a burr.
However if I grind dry, letting the grinding heat change the metal to a straw color, I can finish sharpening this annealed bevel, and roll a nice burr, that cuts just fine. If it holds the edge better before it was annealed, I can't say, but I can say for sure that it is softer.
By the way, I use these scrapers without a tool-rest, grasp it between the thumb and forefinger. I drag my gloved forefinger against the turning to gauge the cut. I only have a small amount past the knuckle, and I work below the centerline, and with a light touch, can change the cutting angle up or down, or skewed on the fly while traversing with a sensitivity that is well beyond anything over the tool-rest that I have mastered.
This is a quick way to remove any against the grain tear-out, and ridges. Rough sanding usually starts at 220 -320.