>3 weeks ago, I sprayed lacquer on several pieces. The shop was 50 degrees at the time. Too cold, I know. But it sprayed well, buffed out nicely and took on a smooth finish.
Last night, I picked up 2 of the pieces and the surface is now rough enough to scratch your skin. Is that the result of spraying in the cold?
>Hi Lan, I use laquer a lot finishing cabinets, never had it do that. If I spray below 60 it will 'orange peel' unless thinned with retarder and sometimes even then. Maybe the wood was still wet?
That sounds like moisture condensation on the wood surface before the finish was sprayed. Now that the surface has been sealed, you should be able to sand it back to smooth, and subsequent coats should be OK.
Just be aware that cold temperatures can also contribute to blushing. That is moisture condensing out of the compressed air. Cold air will not absorb as much moisture as warm air, and the air cools as it expands, causing the moisture to condense and form the blush.
>Years ago, I was making Japanese-style table and wall lanterns as a production item. I had to spray in the middle of January in temps down to 0 degrees, and my only spray booth was an open garage door. What I did was to keep the lamps and the lacquer in the warm shop until I was ready to spray, then take the gun and the piece out to the turntable under the open garage door, spray it, and bring it back into the heated shop to dry. My finishes were just about perfect right off the gun. Maybe it was luck, but I think it was all about having the materials and finish at room temp.
>Thanks everyone. small amounts of moisture seems like the most likely candidate in this case. My in-line water filter is 15 years old. Don't know if those things wear out or not.
This place is still the best education, I have ever recieved.