>I have a hollowform that I have just finished turning and I'm thinking about giving it a tung oil finish.
I have some pure tung oil that I have cut to 30% with mineral spirits. What is the procedure from here? I think I read somewhere that you have to apply a coat, let it dry several days, sand it down and apply another, and so forth. But I'm not sure of the details and what I am trying to achieve at each stage.
What about buffing?
When all is said and done, what is the result? Glossy? Satin? Matte?
>Thanks Carole. That's the article I remember seeing. The tung oil I bought...which is 100% pure but probably not polymerized...suggested, on the can, to use mineral spirits (paint thinner) to thin.
Is there gonna be a difference in the way the tung oil drys or hardens or responds to "cutting" with the steel wool using paint thinner instead of turp?
I'm still wondering about buffing the piece after I've got 3 or 4 coats of tung on it--white rouge and carnuba?
>There is nothing wrong with using Paint Thinner (Mineral Spirits) or Naptha to thin a Tung Oil. The difference is that the Turpentine (the real stuff, not the replacement) leaves behind some natural oils that help keep the polymerized oils and varnishes from becoming brittle with age. The Paint Thinner just evaporates and leaves nothing behind to enhance the finish. Kerosene works similar to Turpentine, with the difference being that the oils are petroleum where those in the Turpentine are natural Pine Oils.
Buffing works well for any oil finish, provided that the wood is saturated and that the finish has fully cured. "Fully cured" means that the finish that has soaked down into the wood with the 1st coat has also polymerized, not just on the surface. With Tung Oil, you can check the surface with 0000-steel wool. If it comes off as a white powder, it has cured. Then give it another week for a full cure. After that, you are just building up a surface film and the steel wool test will be fine.
That's how I do it in North Idaho. We have a 33% Relative Humidity here in the summer, an ideal climate for oil finishes. Others will have different experiences with drying oil finishes because they are in a different climate.
>Thank you Russ, that clarifies things a bit. Even though my tung oil is not polymerized, I take it from your article that everything is the same it just takes a little longer.