I need help with Russ finish

Timmy

>I've mixed that finish that Russ has a recipe for on his site and it just wants to harden on me. Not really harden but get thick like that and all. I asked for some help and guidance sometime back and someone got kind of nasty with me like I wasn't reading things right. Anyway, can anyone help em with this stuff, why is it so thick and not flowing like I figure it should. I really want some help but please don't get nasty or saracastic with me. If thats how you have to answer I might as well just stay confused and you can just stay rude. Thanks guys

Re: I need help with Russ finish

#2

Re: I need help with Russ finish

Carole Valentine

>Hi Timmy,

I have not mixed Russ's recipe yet (tomorrow if my tung oil arrives) but Russ say's this is sort of the homemade equivalent of Waterlox which is what I have been using. I think oxygen is the catalyst and it will gel in the container after it is opened rather quickly. I decanted mine into half cup mason jars, gave each a shot of Bloxygen and sealed them tightly. They are stored in a closed box away from light. How long have you had the finish mixed and how are you storing it?

Re: I need help with Russ finish

#3

Re: I need help with Russ finish

Timmy

>Thanks to you Carol. I only mixed it maybe for a month or a bit longer ago. Its in a big milk jug and maybe air gets to it. That could be it I guess like you said that the air thickens it. Can I save it yet or is it done for now. Man your lots better than the Mark guy and his attitude and all, thanks again to you for all.

Re: I need help with Russ finish

#4

Re: I need help with Russ finish

gary s clarke

>are you using 1/3 each of marine spar varnish, turpentine and tung oil?

Re: I need help with Russ finish

#5

Re: I need help with Russ finish

Timmy

>Hey Gary I'm mixing those thirds but using regular varnish not marine stuff. Is that what causes this problem to be happening do you think? I think its maybe the air thing that carol says is doing it.

Re: I need help with Russ finish

#6

Re: I need help with Russ finish

RussFairfield

>Try mixing your finish in a mason jar with a lid that you can seal. You should be getting a year before it starts to gel, unless the Tung Oil is old. Mixing it in an empty milk jug is abiout the same as leaving it in the open air.

Re: I need help with Russ finish

#7

JL

Re: I need help with Russ finish

JL

>Timmy, use "impermeable" containers, i.e. glass or metal. Milk jugs are made of a type of plastic called HDPE (high density polyethylene. HDPE has a high oxygen transmission rate and the milk jug probably has too much "headspace" (space above the liquid). I like to use mason type jars (1 pint or 1 quart). I keep them sealed until I start to use them.

Re: I need help with Russ finish

#8

Re: I need help with Russ finish

Timmy

>Thanks with muchness to all of you. I will throw this batch away and mix a new one in the container that is suggested. It will be one that seals real good and keeps the air on the outside. You are all nice and my thanks to you again.

Re: I need help with Russ finish

#9

I need help with Russ finish

ob obrien In Pensacola

>Timmy; Sorry some dude was rude. Here's some friendly thoughts for you. Save some of the dishwashing bottles your family dishwasher throws away. Mix up your finish and decant it into the smaller bottles. Now squeeze the bottle till most all the air is out of the bottle and screw the cap on tight. Another solution is to pick up some computer keyboard cleaning spray at say computer depot. It's an inert gas and can be used like the bloxgen to displace air in your cans and jars. For a lot less money than the blogen. Have fun and make something pretty. OB