another oil finishing question

GaryG in MD

>There have been several nice long threads recently about finishing with oil-based products, and I'd like to extend that for one more set of questions.

I would like to hear your thoughts on the practical differences between Waterlox and Minwax Tung Oil Finish. If I'm not mistaken, they are similar products -- an oil and resin mix which first penetrates and then, after 3 or 4 coats, builds up a surface layer as well.

I've read comments from people using one or the other with success. What are the tradeoffs that would make me want to buy or use one over the other for any given circumstance? Or is it just six of one...?

Next, how are these different from Watco Danish Oil?

Finally, I'd like to know what is the benefit of the procedure I've heard about of first using several coats of Watco Danish Oil followed by Waterlox, if they both do about the same thing?

I'm trying to zero in on an SOP, and I'm being confused by all these similar products.

TIA,

Gary

Re: another oil finishing question

#2

Re: another oil finishing question

David Breth

>I typically use Minwax Antique Oil Finish, which is a really close relative of the Minwax Tung Oil. Not too long ago, I tried an experiment, where I had two cups from the same piece of wood. Decided to finish one with Watco Danish (WD from now on) and the other with Minwax Antique Oil (MAOF from now on).

MAOF cup was looking good within a couple of days. I'll say three applications. WD never gained any kind of sheen. I had intended to keep both pieces on the same pace - 48 hours between coats, same number of coats, but eventually gave up on the WD and finished it off with MAOF. No noticeable difference in color between the two, and no noticeable difference in texture between the two.

I know a lot of people really love WD, but the couple of times I've used it I have gone crazy. I'm ok with spending time for a proper finish, but there comes a time when I want to see that proper finish before my own end of life. I have tried soaking a little bit with WD, but I'm just not willing to have gallons of something that costs that much laying around so I can pour it back and forth into buckets.

I would say that's my two cents, but you'd have change coming.

David B.

Re: another oil finishing question

#3

Re: another oil finishing question

RussFairfield

>The short answer to a complex question is that there is no difference.

In the broader definition, all oil finishes are alike because their liquid molecules polymerize into larger solid molecules to form a "finish". We call this "drying", and these oils "drying oils". The resins can be those in the oil itself, or they can be added in the form of either natural or manufactured compounds, that will form a harder surface film than the oil itself. With those definitions, Watco Danish, Waterlox, and the Minwax "Tung Oil", Wipe-On Poly, and "Old Fashioned", are all the same. And, they are no different from any other oil finish that is mixed together as a commercial product, or something we brew up ourselves.

The devil is in the details. Different oils have different properties. There are differences in how they react to light and air, UV resistance, resistance to moisture in the air, resistance to acids, chemical resistance, color change with age, how they change the color of the wood, abrasion resistance, hardness (durability), repairability, cure time, useability, just to name a few.

The common "drying oils" used in finishes are Tung Oil, Linseed Oil, Boiled Linseed Oil, Soybean Oil, Walnut Oil. Tung Oil is naturaly a drying oil. Walnut Oil can be either drying or non-drying, depending on how it was extracted from the nut. Raw Linseed is a surface drying oil that seals the liquid under it from the oxygen it needs to "dry". Boiled Linseed Oil has drying agents added to solve the surface drying problem. Soybean Oil is a non-drying oil that will polymerize in a thin film when exposed to air whith the addition of metallic salts.

Similarly, the different resins will have differences in the same properties as the oils. The resins may be natural resins and gums that are extracted from trees and plants, or they may be a mineral. They may be alaphatic resins that are extracted from animal fat. Then there are the synthetics, the 3 most common being alkyd, polyurethane, and phenolic. Add to that the definition that consideres the solids in the oils themselves as being resins, and the topic of resins starts getting complicated.

This is not a simple topic and there is no simple answer. All are oils, all are different, and those differences will appeal to defferent people. You will have to determine which of the different oils will give you the properties and workability that you want. All we can do is give you our personal preferences.

Here is my view of the products mentioned. There will be those who will argue with every one of them.

I prefer Tung Oil because it doesn't get as dark as fast as Boiled Linseed Oil or Soybean Oil, and it changes the color of the wood the least. And I prefer the phenolic resins for their softer and warmer appearance and feel than the polyurethanes, and they are more durable than the alkyds.

That means I would prefer Waterlox because it is the only one of the finishes listed that contains only Tung Oil, and it is the only one that contains phenolic resins. The finish that I blend myself is as close as I can get to Waterlox, and I make my own because it has the advantages of lower cost, more solids (resins) anmd that means the same results with fewer coats, longer shelf life because I can mix it in smaller quantities as needed, and I have control of how much thinner is used.

Watco Danish is and has always been the finish of choice for a lot of woodworkers and woodturners. It has gone through so many different ownerships and formulations in the last 15 years that it is impossible to tell you what is in it. It started as Boiled Linseed Oil and Mineral Spirits, transitioned through Soybean Oil, went through various blends, and I understand that it has returned to its roots.

Minwax "Tung Oil" finish is the poster-child for the finishing products that have made "Tung Oil" a generic term because the closest they ever got to a Tung Nut was the name on the label. It is possible that the label is not a total falsehood because there might be some resins added that were extracted from the Tung nut. There is nothing wrong with it as a finish, and a lot of people are using it. Just don't get the notion that you are using Tung Oil.

Minwax Poly. The oil used to be soybean, but I have no idea what it is now; and the resins that are added are polyurethane with all of the properties that go with it. I personally don't like polyurethane resins, so this wouldn't be a finish that I would use. There are a lot of woodturners who disagree with me.

Minwax "Old Fashioned Oil Finish" (in the red can). This the only one that lives up to its name. It is, and has always been, a high quality Boiled Linseed finish; and that's not at all a bad thing. This is the most under-rated of all the commercial finish among woodturners.

Whew.

Sorry it got so long.

Re: another oil finishing question

#4

Re: Correction

RussFairfield

>I used the wrong name. What I called "Old Fashioned" is really the "Antique Oil" that David refers to.

Re: another oil finishing question

#5

Re: another oil finishing question

Wally Dickerman in Arizona

>Very informative Russ. Thanks. I've used Daly's products for many years, and I know that you do also. How would you rate Daly's Ben Matte and Seafin oil finishes?

Wally

Re: another oil finishing question

#6

Re: another oil finishing question

RussFairfield

>Daly's is every bit the equal of Waterlox, and for about half the price. And for some reason they keep longer after the can has been opened.

Re: another oil finishing question

#7

Re: whew

GaryG in MD

>Thank you Russ. Outstanding answer, as always. You did such a good job on this that I seriously think you should move it over and save it as a "WC Article". It is certainly general enough. I appreciate your time and experience. ...Gary

Re: another oil finishing question

#8

Re: another oil finishing question

GaryG in MD

>Thanks for your reply David. I am having exactly the same experience. I have several face-grain pieces with 4 coats of WD which are just starting to get a sheen (and they were 'liberal', soaking coats. I have an end-grain finial which has about 10 coats and is still dull. I'm going to finish them with the MTOF I have here on-hand now, but I'm also going to look into getting the Daly's per Wally/Russ, or Waterlox. ...Gary

Re: another oil finishing question

#9

Different Waterlox products

TD

>Gary, there are several (5) Waterlox products available in color coded cans. The green can is the fastest finish they have but it builds on the surface. The red can is more of a penetrating finish that gives a better, but slower, "in the wood" finish. They also have an Antique oil finish and a Marine use finish. The red can is somewhat like the Minwax Tung Oil Finish. You can save a lot of money by mixing your own oil for sanding and then going to one of the above oils for the final 2 or 3 coats.

TD

Re: another oil finishing question

#10

Re: Different Waterlox products

GaryG in MD

>Good points, Terry. Thanks. ...Gary