Howard Pollack

I just acquired a Sigma Power 6000 stone, the pink speckled one. I got it from Japan and I don't have any instructions vis-a-vis water. Is that stone splash-and-go or does one need to soak it? Thanks. -Howard

Re: Sigma Power 6000 question

#2

Re: Sigma Power 6000 question

Orlando in So. Fl.

I have the same stone. It's a splash and go. Wet it to flatten it then it's splash and go. It's one of the "hard" ceramic Sigma stones that has a binder while the Select II does not have a binder. I use it as a medium stone then go to the 8K of the same type, finished by the 13K. But I also use oil stones to sharpen and now that I have experienced the "unicorn effect" I'll probably will use all of the sharpening mediums I have. I'm retired and not a professional woodworker, so I have the time to experiment. :)

Re: Sigma Power 6000 question

#3

Re: Sigma Power 6000 question

Don Peters

I got one from Schtoo about five years ago, pinkish with dark speckles. It's a pretty hard stone for 6000 grit, so it doesn't easily catch divots. It likes to be wet; I usually soak for 15 - 30 minutes, and I leave it in the pond during the day, maybe two to six hours. It's hard, and not very fast, so I slurry briefly with a 400 grit diamond plate before first use and thereafter as required.

I always air dry waterstones evenly; I'm in Arizona, and everything's dry anyway. And, as schit happens, when I pulled that Sigma out of the pond at the end of the day to dry it, it broke across it's width. No trauma or shock, it just went, "klink". Raggedy fracture, but no missing bits. I dried it for about a week - did I mention Aridzona? - then epoxied it back together. The ragged fracture line helped get it close it's original shape/flatness, but it's not perfect, and I'm still working on flattening it. So that's my experience with this stone.

I should mention that I've used both powered and manual waterstones since about 1977. They've all been man-made, so the following only applies to man made-stones. I've had several failures, about half of them my fault, and the other half "unexplained". So all that probably just muddies the waters. Did I cause the issues with those unexplained fractures? Maybe. I'd appreciate your opinions. In the mean time, I think it's like most things in life: it's a crap shoot. Schit's gonna happen. But I'm still using that stone.

Re: Sigma Power 6000 question

#4

Re: Sigma Power 6000 question

Winston

I don't soak mine, but I wouldn't exactly call it a splash-and-go stone. When it's dry and I go to use it, I put water on it and it soaks it all up within 10 seconds. I have to do this many times (maybe 10 or so?) before it stops soaking up water, and the water will just sit on top of the stone.

This is different from, say, Shaptons, which really are splash and go.

I should go find a plastic bin to soak it in for a minute or two before using it, but that's actually nontrivial for this stone. It's mounted to a wooden base, which complicates things a bit. The options are to put it upside-down in the bin, or right-side-up. If I put it in upside-down, then it soaks in water very slowly because the entire top surface of the stone is contacting the bottom of the bin. If I put it in right-side-up, then I need to find a tall bin and fill it with lots of water, because of the extra height from the wooden base. (Maybe I should try to figure out how to separate it from the base.)

Re: Sigma Power 6000 question

#5

Re: Sigma Power 6000 question

Curt Putnam

More than a splash and less than a soak. Mine, too, is mounted so I use a small bottle (like a standard squeeze bottle) to spread water on the surface. I do this while working on the 1000 grit stone and then again before each use. Works for me.

Re: Sigma Power 6000 question

#6

Re: Sigma Power 6000 question

Orlando in So. Fl.

To clarify my statement of splash and go, I do what Winston and Curt do when I initially start to to use it. I get it nice and wet, I don't soak it for an extended period of time, and flatten it if necessary. I then keep it wet while in use, which is what I meant by splash and go. The other time it gets dunked is if/when I have to flatten it after some use.

Re: Sigma Power 6000 question

#7

Re: Sigma Power 6000 question

Jaap

I've been using the Sigma Power ceramic 6k (aka jinzo renge suita) for several years, I'm on my second one actually. It performs better when you permanently store it in water and it doesn't have any detrimental effect on the stone.

Btw, the orange Select II 6k does have a binder. Not much though and it's very friable when used on soft steels. A small piece of Select II 6k also makes an outstanding nagura for the ceramic 6k.

Re: Sigma Power 6000 question

#8

you're right....

Orlando in So. Fl.

....about leaving them in water but it's not what I prefer to do. Stu mentioned that Sigma Power Ceramics below 4K should be soaked but above that it's not required.

ALL Sigma Power stones can be left in water. The Select II shouldn't be left to freeze (until I learn otherwise) but the ceramics aren't harmed by hard freezing as far as I have found.

Sigma Power stones do require soaking below #4000 grit, but above that (#6000 and above) do not require soaking at all.