I'm new to buffing wheels. Instructions with the one I bought recommends dressing the wheel with tallow or similar "hard fat" to facilitate adherence of the buffing compound. I know nothing about "hard fat", so I applied some honing oil to the wheel before charging it with compound. It worked, but it's messy. What do you use?
I think a lot of the buffing setups charge the wheel fully to speed up a large buffing project/area and keep the abrasive in the wheel longer.
We don't really need to do that. My preference (and it's subject to someone coming up with something better) is just to take the buffing bar of choice, stick it into the wheel for a second or two and then re-do every couple of items buffed. It hasn't to this point built up in any of the wheels that I have (any mass of rotating fat could actually deflect an edge, too).
What little I know of buffing (and it is little) is that the wheels go from loose to basically rolling thunder (we're choosing something in between) and the amount of compound can go from almost nothing, and transient to "greaseless" compounds (for coarse work) that are basically a glue intended to stick with the wheel rather than be more transient.
If a wheel loads, there are combs to strip some of the material out of the wheel, but I don't have one and haven't needed one yet. start slow would be my advice, and just with the buffing bar (no pre-conditioning the wheel - we like the soft gentle nature of the wheel - it gives a lot of flexibility).
I am bashing out drawers today. Unicorned the required chisels. Prepared chisels as usual except lowered bevel angle from 30 to 25 degrees. Touched stick to wheel for 2 seconds +/-. Touched chisels to wheel for 3 seconds+/-. The bright glint of light at the very tip says its done and good enough.
The convex bevel acts as a convex mirror under a light source. The bright, narrow band can not be missed if it is there and it doesn't take much to apply it.
Important point. You want the wheel fluff—the stuff that hits the blade—to have very little to no body to it. The fluff with no bidy will just lick the edge; it will select for the edge, and just the edge. Which is what you want—you want the rounding limited to just the first few thousandths of the edge.
But when the wheel gets loaded and develops some body, it now has striking force. It won’t limit itself to the edge—it will take metal off whatever it hits and proportionate to wheel speed. So instead of getting a unicorn, you get a rounding extending 10-15 thousandths up the edge, rather than 3-5 thousandths.
In other words, what David said....keep the edge fluff loose by applying sparingly to start and go from there. Loading up will make the wheel too aggressive.
This is about the buffing stick and the carrier for its abrasive. I currently have two Dico Premium Buffing Compositions charging sticks, E5 (emory) and SCR (stainless steel) intended for buffing ferrous metals. I have found they also work well with my cotton buffing wheels for polishing brass and bronze.
I also have some Norton 0.5 µ diamonds suspended in water (in a syringe from Joel at TFWW), but I strongly suspect the diamonds are inappropriate (to say the least) for polishing an Equus monoceros, since I suspect the primary function of the unicorn process is to fuse the deep, sharp scratches left in the carbides and other crystals that cause premature edge failure due to fracture concentration and extension.
If I can, I'd prefer using the materials I already have at hand, instead of going down a new, unfamiliar rabbit hole. For consistency, I would like to charge my buffing wheel with the same abrasive as I charge my leather strop and hardwood slips. For these, I have 0.3 µ powdered Cr2O3 that I mixed with a mineral oil carrier and that I apply from a Monoject 412 syringe. While that works for a leather strop, I don't think it is appropriate for a Unicorn Buffing Stick. I would like to make my own "green crayon."
Has anyone made a DIY buffing stick? Can you recommend a carrier (maybe beeswax?) and a method for mixing the chromium oxide and forming the stick, getting it out of the mold and packaging it for use?
I just made one with paraffin - something like 2/3rds paraffin and 1/3rd abrasive. I think it would be better (by weight) if the two were switched. I have way more wax than needed, but no significant detriment at this point.
Bill suggested beeswax. I think many things would work. If too waxy loads the wheel, then combing the wheel should fling most of the nasties out (tip above to use a spent rasp is a good one).
Agree with using what's on hand.
(interestingly enough, iwasaki used felt or something of the sort with 1 micron diamonds in it about 50 years go when such things would've been expensive - after an uber expensive super premium japanese natural waterstone. He said the comfort of the shave was improved afterwards, the edge was relaxed a little bit and improved. I was horrified to see that as i'd tried fine diamonds on a razor on a harder surface and it was bad. But have learned since, the felt and diamonds are probably a magic combination. I don't think aggressive stuff would be a problem on the wheel, but it would be a waste as the wheel will fling out and then subsequently consume more in the next charge. While it's wasteful, I'm also sure that most people would never use a $14 jackson lea green buffing bar in their lifetime)
Thanks, Monty. That's just the sort of information I was looking for. It brought back memories of my misadventure in filling a syringe with compound. His method, as he points out, is very expensive for making a single use mold. I'll need to think about that one for a while. I need to make sure I come up with something ingenious (like Wright's carbonite ) and not really, really stupid. Speaking of stupid, I once tried to make a beeswax applicator from an old stick deodorant container, but it was totally unsuccessful, because I couldn't figure out how to get the wax to release, and I stripped the threads on the extension screw.
..any plastic package that anything comes in will do for a mould. Beeswax or paraffin can be held in the jaws of a pair of pliers (hold tight as the hold shrinks!!) and the wax torched off to drip into a container already full of abrasive.
The wax cools a little bit but stays easily liquid enough to mix for a while and it's not close to hot enough to be a problem with the plastic (low temp wax has to be chosen, but it "Runs" away from the torch flame long before it ever gets that warm. Then you can just peel the plastic off and throw it away.
This is lowbrow and can make funny looking buffing bars, but they work. I'll find out later if paraffin is a bad choice for the wheel, but many things were a bad choice for oilstones in the past and there's plenty around to just simply remove oxidized material (or diamond hone it off).
The total time spent for this process is about 3 minutes, but some planning ahead is worthwhile as all I had was a blister package for a fishing rod combo that I bought for the kids.
If you have to have a specific shape "Crayon," Don Williams has demonstrated another trick for containing either the stick itself or the mold material: Lego blocks! The problem there is it may take me quite a while to find my Legos. They're somewhere in storage on the other side of town.
If you haven't watched the video that Monty provided, as the youtuber added the beeswax to the powdered abrasive, I thought I didn't particularly like that idea because he was going to have some difficulty getting a consistent mixture. He immediately noted that he should have added the powder to the melted beeswax, and I just nodded my head. One thing I like about amateur YTs is that I can often learn important lessons from the results of their less than optimal procedures, that I would never see in professionally produced videos (or even in books) by experts who have perfected their procedures.
...and I really don't know what any other place does, but it does look like they pour the bars into open moulds because the bottoms look like a liquid that partially settles in place.
Which means the mix is made and then poured into the mould.
In the case of linde A, it's so light weight that it really doesn't matter what order you go. I don't actually have a clue when the particle size would be big enough for it to matter. I put the linde A in my tray first and then dribbled the wax into it, and then stirred until it was uniformly white. It stayed that way.
Since coarser bars aren't hard to find really cheap, I've got no intention to make them (I don't think they could be made as cheaply as they can be bought), but I didn't see a linde A bar!! and I have a lot of linde A now that isn't going to be used.