david weaver

I've been waiting for a while to get one of these irons. I don't *think* I already have one, but you never know.

It's titled Revilo High Speed Steel, and these are the earliest HSS irons that I am aware of. They show up with some regularity as replacement irons in infill planes, and they're usually little used, but the price tag for ratty infill planes that I usually see them in negates my desire to buy them just to get the iron.

In this case, though, someone stuffed this 55mm iron in a coffin smoother (it's a parallel iron) and sold the whole lot for $15.

It'll be interesting to see what the HSS is. I'm hoping that these were made at a time that HSS was generally tungsten HSS , but I don't see a lot of history anywhere about the company that made them.

One thing of note is that over the years, I've seen about a dozen of these irons for sale. All but one were nearly full length, which is uncommon for parallel irons. I'm guessing that they were set aside due to lack of power grinding.


Re: Revilo High Speed Steel Iron

#2

The maker - F. Mountford and Sons

david weaver

Is listed in English trade manufacturers listings at least as long as 1893-1925.

They're listed as a "scythe manufacturer" with no other references (toolmaker, etc) in the lists that I can find.

Re: Revilo High Speed Steel Iron

#3

Very likely Tungsten

Patrick Chase

Based on the active date range you give for the maker, the steel would almost have to be Tungsten based, i.e. T1 or one of its non-standardized forerunners. Molybdenum-based HSS didn't become common until WWII.

If it's actually branded as "High Speed Steel" then that dates it to the 20th Century.

Re: Revilo High Speed Steel Iron

#4

Nice Iron - soft for HSS

david weaver

My iron came Friday.

I put it on the sandpaper lap today and set up the back, and set up the cap not thinking (it's a woody cap, it won't work under a lever cap, though one could grind the brass boss off).

I have a couple of planes that take a 2 1/4 iron, but I like this beater A13 norris. they are never cheap, but the condition of this one made it cheaper, and it's a lovely plane.

The revilo iron is soft for HSS (which is intentional, I'm sure, given the era), and other than having a slightly more persistent wire edge, it's smooth sharpening and will even raise a wire edge on an oilstone.

Due to the infill work, I didn't have a chance to do more than a few heavy smoother shavings, but the feel is excellent so far. I'm pleasantly surprised.