Water stone for PM-V11

#1

Water stone for PM-V11

Josko Catipovic

I've upgraded most of my plane blades to PM-V11 and am struggling a bit more than expected with my King water stones. I grind on a Tormek, then 1200 and 8000 Kings.

I saw the LV writeup on water stones, and stuff about Shapton, Sigma, Bester, etc. but am hoping that someone with first-hand experience with PM-V11 would share what works. Thanks in advance.

Re: Water stone for PM-V11

#2

Re: Water stone for PM-V11

david weaver

All of the above work. The king 1200 might be a little slow, but the 8k should be fine if you're microbeveling.

I'd probably first add a bester 1200 (if you don't mind soaking, it is a stone that can't be used without soaking) or a shapton pro 1000 as a first stone, and if that doesn't satisfy, an ezelap 600.

I found it a lot like sharpening hard A2 - the key to keeping things easy is using the grinder more often and doing less work with the stones.

I manage to sharpen it on a washita stone just fine (I don't use it much, but when I do), but it takes a little more work with it.

Re: Water stone for PM-V11

#3

Re: Water stone for PM-V11

Derek Cohen (in Perth, Australia)

Hi Josko

The system I have is very successful: Shapton Pro 1000, Sigma 6000 and Sigma 13000. I often also finish with Lee Valley green compound applied to hardwood.

With a hollow grind, the entire honing of a blade should not take more than 60 seconds!

Regards from Perth

Derek

Re: Water stone for PM-V11

#4

Re: Water stone for PM-V11

Josko Catipovic

Thanks guys. I should have said my biggest surprise is the amount of time I have to spend reflattening the 1200 King, and how easy it is to loose control of blade camber with it.

Sounds like the 1000 Shapton is worth looking into next.