Bill Tindall, E.Tn.



I have a King that I use for kitchen knives. It was hollowed 1/8". I flooded an 80 grit sanding screen with water and rubbed the stone on the screen. In an amazing less than 5 min the hollow was gone.

These screens are silicon carbide which is harder than most abrasives other than diamond. The open mesh cuts fast. Now I have a red puddle on the driveway.

Re: Rapid flatening of waterstone

#2

Re: Rapid flatening of waterstone

TomD

I have a particular cement block that is flat, and just rub it directly on that, keeps them flat when they are way out. The method I use more generally is I have 2 800 stones and just rub them together, then I flatten those that are finer 1500 on 800, 4K on 1500, and so forth. Some say you contaminate the stones and you won't get good results, but I learned this method from close to the source and have had good results with it.

Of course, using techniques that don't hollow is a good practice to follow.

Re: Rapid flatening of waterstone

#3

Re: Rapid flatening of waterstone

Derek Cohen (in Perth, Australia)

That's what I used 20 years ago: a length of 120 grit dry wall mesh on formica for King stones. It worked very well.


Regards from Perth

Derek

Re: Rapid flatening of waterstone

#4

question and comment

Bill Tindall, E.Tn.

Does the mesh work well for the more modern ceramic water stones that most people now use? It certainly is cheaper than the diamond plates I hear of others using, and on the King, a lot faster. It would have been useful to tell us why you changed to something else, if you did, or not.

Looks like your arrangement didn't use water. Flooding the mesh with water greatly increased the cutting speed. Also I am using 80 grit.

Re: Rapid flatening of waterstone

#5

Re: question and comment

Derek Cohen (in Perth, Australia)

Hi Bill

I gave up on the mesh when I moved from King to Shaptons. At that point I switched to a DMT extra coarse diamond stone for flattening. I still have it.

The mesh was used with water. The way I did it was to take the wet stone to the mesh. Water and waste could be wiped away by lifting the loose end of the mesh (the other end was fixed). It was a useful system.



Regards from Perth

Derek

Re: Rapid flatening of waterstone

#6

Re: question and comment

TomD

I used DMT back in the day when they were still integral plastic blocks. Kings ate DMT alive since diamonds are harder than Kings, but Kings are harder than the vitrious bonding material with which DMTs are assembled. I have used Shaptons, but never saw the benefit to moving up to them. Kinda funny at the time shaptons became all the rage so were natural stones, so soft can't be that evil.