Well you don't say what you are using it for...
Here you can see the T-88 being mixed at around 12:00:
http://www.youtube.com/watch?v=PXd11KC07ZE
It is a pretty typical 2 part mix out of bottles where it is stiff enough to go up the stick as you mix.
Comparatively West is wet like maple syrup, or corn syrop.
There are far runnier epoxies still, particularly those modified for application over cloth with a roller (west works great on cloth but you have to spread it with a squeegee.
The thing is that while WEST is far runnier that T-88, WEST is normally used with a range of products to modify it characteristics. These include colloidal silica which stiffens it and cuts running dead in it's tracks. CS if overused will lead to a hard to sand, brittle, heavier epoxy glue, that yields poorly. But there are other products like microballoons that can be added to extend the mix, give large batches, that are lighter syntactic foams. So a recipe I use a lot is 3 parts micro balloons to 1 part silica. Not to say that you can't just use WEST without these additives.
Basically, if you have used 5 minute epoxy and found the consistency useful for what you are currently doing, T-88 is like that. That is why guys use it to spot weld stuff like the airplane components. WEST is great for projects where you need a thinner glue, and particularly a glue that will be strong and versatile. It can be used as a coating, sealer, lamination resin, glue, casting parts, harware bonding, fabric wet-out etc...
West is similar (better than) Sytem three's classic resin, they offer several products that are in the range (they bought up a bunch of brands). S3 stuff, and indeed sometimes west are offered in trial pack size. With T-88 (one of the brands S3 bought up) it is already in smaller packs. MAS is another you might find a trial pack in.