Re: The Chair - End of Phase One

#2

Jack Guzman from Maine

Re: The Chair - End of Phase One

Jack Guzman from Maine

Derek,the figure in that wood is amazing. You mention excessive heat. The temperature outside when I went down to my shop this morning was -4 deg F. It has since heated up to about 10 deg. Been like this all week.---Jack

Re: The Chair - End of Phase One

#3

Re: The Chair - End of Phase One

Tom in Toronto

On the epoxy, you can keep it cool in a cup of water or some such, or mix it in a shallow aspect ratio container. The runny spill I stop by masking around the joint reasonably carefully. And by adding colloidal to the mix. Depending on the wood, you can use the raw epoxy on all surfaces to the depth of a first coat of finish, then you bulk up with the colloidal, and apply that from the rest. Once you are used to using this stuff you can run through the steps fast.

For mixing small amount I get suitable container, either plump pop bottles or squeeze bottles. I drill a 3 mm hole in the cap, and insert a PD dose syringe. you can accurately and cleanly meter West with this rig. The PD dose trick came from Michael Fortune.

http://www.amazon.com/Ezy-Dose-Syringes-Dosage-Korcs/dp/B000VCF6FG

http://www.squirrelsandmore.com/rehab-supplies/oring-syringes.html

I use these for everything when I can find them. YOu will see them in dish soap bottles, mouth wash, etc... THe oring means they don't separate, and the syringes go on and on.

Re: The Chair - End of Phase One

#4

Re: The Chair - End of Phase One

Tom in Toronto

Oh by the way, I use the 5cc ones that the squirrel place seems to be out of, and I use the non locking tip.

Re: The Chair - End of Phase One

#5

Re: The Chair - End of Phase One

Tom in Toronto

And there are cool valves that work with these so you can make pumps. Does anyone know a place that has all this stuff, is cheap, and easy to deal with like paypal no data collection?

Re: The Chair - End of Phase One

#6

Re: The Chair - End of Phase One

Bruce McCrory

Your wood grain is all shaky! Didn't you sand everything smooth? :D

Gorgeous!

Re: The Chair - End of Phase One

#7

Re: The Chair - End of Phase One

Sgian Dubh

Nice work so far Derek, But I do have one comment. You mention stretchers a few times in your write up but there are no stretchers in your chair that I can see. There are four rails connecting the legs plainly visible, but looking below the rails for those mythical stretchers reveals only open space.

The chair below has stretchers set set just below the rails which is somewhat uncommon. The placement of stretchers in chairs tends to be much lower, typically the bottom edge is 50 - 100 mm off the ground, but there's no hard and fast rule that I'm aware of for their position. Slainte


img

Re: The Chair - End of Phase One

#8

Re: The Chair - End of Phase One

Derek Cohen (in Perth, Australia)

Hi Richard

Yes .. I realised shortly after I began using "stretcher" that I should rather have used "rail". However no one said anything! And then I just continued for continuity sake.

Just another word :)

Regards from Perth

Derek

Re: The Chair - End of Phase One

#9

Epoxy for Tom

Derek Cohen (in Perth, Australia)

Hi Tom

I could have done with some of those syringes with measurements. I could not find any and had to make do with marking off with blue tape!


I just snapped a picture of a couple of bottles of West System. A few months ago I was laminating a few curves pieces, and the epoxy did not cure. I probably did not get the mix correct, but was not sure if this was due to the pump in the bottle or whether I miscounted the number of pumps used for the mix. To be safe, this time around, I used the syringes to measure the resin and hardener.


Regards from Perth

Derek

Re: The Chair - End of Phase One

#10

Re: Epoxy for Tom

William Duffield, on the Cohansey

West System also supplies a #209 hardener, which is very slow, but you still may not find it slow enough for 111°F or so.

http://www.westsystem.com/ss/209-extra-slow-hardener/

When I use disposable syringes like that (my weapon of choice), I have found that I must really treat them as disposable. Trying to reuse them by cleaning with acetone or mineral spirits is an exercise in futility. The stoppers swell and soften, and pull loose from the plunger, wasting the epoxy and upsetting my timing.

You can also measure West System by weight. I use a postal scale or another, smaller electronic scale (about the size of a calculator) that is accurate to 0.1 gram. I find I lose track of number of pumps all too easily, and if the pumps haven't been used in a while, they might have developed air bubbles, which really messes up the measure. If I'm mixing large enough batches to need to rely on the pumps, I usually pump one measure into a clean cup, set it aside and pour it back into the can when I'm done measuring. (Just don't mix up the cup of hardener with the cup of resin!)

Re: The Chair - End of Phase One

#11

Re: Epoxy for Tom

Tom in Toronto

That is why one needs to use the oring syringes, it depends on the materials, but they can remain in use for as much as year or more. While I only get a few days out of the cartridge ones.

I use the postal scales also, though the +- .2g is not so great for small amounts. There are grain scales.

Derek, my general experience with the west pumps is that they keep dispensing epoxy accurately all the way to the point were they stop working at all. There is a tendency for all these pumps to carry bubbles, but we seem to be able to estimate past those. The key thing with the pumps is to not get distracted at all. In boat building it can be real cash to waste a batch, but if we don't know for sure what happened we chuck it, or on some occasions there can be a secondary use. 3% error affects WEST strength.

I have plans for a pump that is rebuildable, and dispenses one measured squirt of both part per pump, but I haven't made one yet.

Re: The Chair - End of Phase One

#12

Re: Epoxy for Tom

Tom in Toronto

Actually, a pretty easy method for mixing small (but more than this project would need) amounts, is to secure a straight sided container, and mark a line on a stick that is volumetrically correct. So you pour in 5 cm, then add a further cm for the hardener. This method is accurate, if you can see into the container, and follow the tide line.

The Gougeons have a method of two circles that makes about 1 tsp. You draw out the two circles on paper, then flood the surface with enough drops to fill each circle, the method takes into account the relative surface tensions of the material. But I prefer the Syringes.

As was probably mentioned, epoxy component weight and volume are not neatly comparable. So you need to get the actual weight that corresponds to the 5-1 volumetric ratio, and the same for any other brands you use.

Re: The Chair - End of Phase One

#13

Re: The Chair - End of Phase One

Don Emmerling

I really like your progress reports on this chair. You must feel very good getting it to this point and in such fine shape. Your work speaks for itself.

Don