1. In re-studying the Kawai paper on setting the cap iron distance I think he is suggesting using the shaving compression as a response for optimum cap iron setting. The shaving should be compressed a bit but not Accordion shaped. It remains unclear to me how the cap iron to blade tip distance is actually (and practically) being adjusted to achieve this happy state.
2. there is another series of papers by Akinori Yamashita , Faculty of Education, Shimane University. I have a copy of the 4th paper in a series of papers and it deals with chip discharge from the plane as the cap iron and mouth distances and angles are being varied. It is dated 1980. Apparently there was a lot of activity studying planing in Japan in the 1980's.
Mitigation of torn grain is demonstrated for "close" cap iron settings. They show in a picture how the grain tears when the blade tip encounters the more dense late, or "summer" wood (hard growth ring), in their test specimen. A distance of 0.1 mm eliminated tear out and 0.3 mm didn't. The bulk of the paper seems to be dealing with shaving clearance.
They derive a formula for calculating throat clearance. The space the shaving has to escape depends on cap iron to blade tip distance, angle of the throat edge facing bade(they conclude 90 degrees is best), bedding angle, distance from bade tip to edge of throat, height of front face on cap iron, and shaving thickness.
This series of papers looks to be interesting and at least the one I have has an excellent English abstract and English translation of the Figures. I will see if I can find the others in this series.