New WoodChat!
Home Articles Forums Gallery Marketplace Videos

WoodCentral Forums

Knowledge You Can Build On — Est. 1998

Combination Press Plough Plane

1/4" SKEW

Posts

1/4" SKEW

#1

1/4" SKEW

Nick Tuzzolino

The skew is for turning, obviously, but you hand tool fellows probably have a broader area of metal knowledge than the turners.

So, I want to make a small 1/4" skew. Can I use water hardening drill rod, grind to specs, and just use it. Or is there more involved?

Re: 1/4" SKEW

#2

Re: 1/4" SKEW

Bruce, a MN Galoot

Most of the drill rod I've used comes annealed, so you'd have to harden it, too. But with W-1 that's not hard.

Re: 1/4" SKEW

#3

Re: 1/4" SKEW

Bob Hackett

For rolling small details like beads you may be better off buying a 1/4" rod of HSS and grinding your bevels on the end of that.Much more user friendly and no heat treating needed. :D

Re: 1/4" SKEW

#5

Re: 1/4" SKEW

Nick Tuzzolino

Shows how much I know about metal working. High speed steel is what I had in mind. Duh!. THANKS!! to all. I have a metal/machine shop supply nearby.

Re: 1/4" SKEW

#6

Moses Yoder

Re: 1/4" SKEW

Moses Yoder

If you grind metal that is already hardened you have to keep it cool enough during the grinding that it will not lose it's temper. The best way to do this is by grinding it a little bit then wrapping your palm around the tip until cool, etc. ad infinitum. Supposedly if you dip it in water to cool it can cause very minute fractures in the steel, although I have used this method also.

Re: 1/4" SKEW

#7

David Barnett

Actually, you can grind HSS to red heat...

David Barnett

...without diminishing its toughness or drawing its temper.