>I have been using McCloskey's Man of War Marine Spar Varnish with good results. But now that the price is over $60.00 a gallon I am looking for another commercially produced non-urethane varnish of similar quality.
Anyone have experience with 'Tried and True'? Or are there others on the market that compare?
The Tried and True varnish oil is a nice product, but does not behave like the spar varnish you are used to. You have to apply VERY THIN coats of the T&T products and they do take a lot of time to cure if you don't. Addition of driers can help, but thin coats are still best with T&T.
Michael Stadulis in Southern NJ, near Philadelphia
Michael Stadulis in Southern NJ, near Philadelphia
Guest
Re: Varnish question
Michael Stadulis in Southern NJ, near Philadelphia
>Steven,
T&T is a modified BLO. It is not used nor will it behave like a conventional modern day varnish. I'm not sure why they describe it the way that they do, but I can't tell that it has "other resins" added.
Having said that its a nice product but not at all similar to McCloskey's MOW.
>The varnish oil does have aresin in it, apparently a natural resin. I swear by it (instant old look to cherry), but I also add tung oil to it (about 25%) for extra resistance. I refinish all my mid-century Danish "antiques" that I like to buy, including my kitchen table, and I find it more resistant than any varnish under heavy use (again, with the tung oil). However, I also think it'll be more ezxpensive than $60 a gallon...at least where I buy it. I add pure tung oil, but if you want it to dry more quickly, I'm sure you could add polymerized tung oil.
>Fine Woodworking compared exterior varnishes earlier this year (May/June Issue). The clear favorite I recall was Epiphanes High Gloss Marine Varnish. However, I suspect is cost even more that what your currently using.
>Historically, varnish was a mixture of a hard resin-copal, amber, etc.- and oil such as linseed. The portion of hard resin to soft oil determined it use. Lots of oil resulted in a soft flexible finish good for outdoors while more resin resulted in a hard finish that could be rubbed out.
Now days the resin is a synthetic polymer. I don't recall ever seeing pine rosin used in a recipe.
Yes, violin makers use rosin to make violin varnish, at least some of them do. I understand there are various recipes, but here are two of the more common ones. I've included here a link from the firm WoodFinishing Enterprises. They have it as information on their finishing products website. Disclaimer: I have purchased from them in the past and I like their service and products. Other than that, I have no affiliation.
There are other rosin-based recipes, but you have to ask a violin maker directly and hope for a direct answer!
>My reason for asking is because a friend uses at least 10 gallons of McCloskey's a year and the increase in price was a concern. I have since found out from folks here that sixty dollars is probably not a bad price.
I like the McCloskey's gloss spar varnish for mixing with asphaltum for japanning as it is handy and mixes well and it is already made up.
I myself have been making my own varnish for the past several years and have made copal varnish, a sandarac and amber varnish and even turpentine varnish among others. I recently found a recipe for the legendary 'Vernice Martin' and hope to mix some of that up soon.
My early varnishes were quite thin but worked with several coats, lately I have been using thickened linseed oil and have been fusing my resins, so the varnish has a much thicker consistency.
I also use spirit varnish (they contain no oil) from various old recipes and they work for light duty applications.