lightfastness of mahogany colorants *LINK*
Bill Tindall, E.TN
>http://www.woodcentral.com/cgi-bin/messages3.pl?read=367857
lightfastness of mahogany colorants
Knowledge You Can Build On — Est. 1998
lightfastness of mahogany colorants *LINK*
Bill Tindall, E.TN
>http://www.woodcentral.com/cgi-bin/messages3.pl?read=367857
lightfastness of mahogany colorants
Re: lightfastness of mahogany colorants
Dean J in MN
>Thanks for sharing Bill!
Re: lightfastness of mahogany colorants
"RJ" Whelan
>Bill ... I have been very pleased with Trans Tint dyes from Homesteading Finishing (Jeff Jewett).
I've been using them for a little over two years and, so far, color fastness has been great.
They can be mixed with either water (distilled is safest) or denatured alcohol as a solvent at a ratio of 1:16 (full strength).
For Honduras mahogany I like orange (at full strength - 1:16) followed by brown mahogany (at less than full strength - 1:22). I use distilled water as a solvent and I preraise the grain with a fairly liberal application of tap water - I test the MC before raising the grain and I let the piece set until it returns to the same MC (generally overnight). I apply the orange first and give it a full day to dry. Then the brown mahogany followed by another full day of drying. I burnish the surface with a fine abrasive pad to knock down any residual raised grain before applying the first coat of finish (usually blonde shellac).
I've used this colorant on two large entertainment centers and although I would prefer leaving the wood natural to darken with light exposure, I must say that I was pretty pleased with the results.
Good luck with your project .......... rj