Kicking a Dead Horse*
Stephen Shepherd in the State of Deseret
>I hate to bring up the subject of Hide Glue fracture tests again but I got thinking about some of the responses to the other threads about the value of this test and you just don't encounter this joint in normal woodworking.
This got me thinking, well of course you do, consider a narrow pin half blind dovetailed drawer front. The orientation of end grain to side grain is greater than 50% in some cases.
Also mortise and tenon joints has a large percentage of end grain / side grain orientation. So these joint tests are important, if do nothing but to raise the thinking about the qualities of hide glue.
This one was sized but I did not allow it to dry. It was harder to break as the pieces were shorter and the failure of substrate looks like a little more than the last, too close to call without the statisticians.
Liquid hide glue is an excellent all purpose adhesive that every woodworker should try and use. If you want to go the extra effort and get a glue pot and some 192g ground hide glue (from Joel), then give it a try.
If you don't want to go to the bother initially then pick up a bottle of Patrick Edwards Old Brown Glue or Franklin/Titebond Liquid Hide Glue and use the best glue in history.
Stephen
(* no offense Todd)