cyano-acrylate finish
Dean Lapinel
>Any good references as to the use of cyano-acrylate for a High gloss durable finish on small wood projects?
Thanks!
Knowledge You Can Build On — Est. 1998
cyano-acrylate finish
Dean Lapinel
>Any good references as to the use of cyano-acrylate for a High gloss durable finish on small wood projects?
Thanks!
Re: cyano-acrylate finish
ThomD
>Tons I am guessing in lutherie. It depends whether the part is of the type that catalyses instantly or not. Rosewoods etc... do catalyze the glue instantly, that makes the process very much like French polishing because the glue sets up as you wipe it on. I take a small piece of cloth and roll it back on itself so there is one smooth hard surface like a fad used in polishing. Then a pour a drop of Hot Stuff thin on it and wipe that on the piece. I just drag it across. Usually you won't get far at the beginning, because there isn't much glue on there. I keep going back and forth until it dries, which can be almost at once. I'm trying to spread it out not get more on top of itself. If you don't let the pad stick, it won't catch on the piece. reload do it again, and just keep at it until it is covered. A lot of glue in the pad can cause it to catch on fire though I have never come close and that would seem to be wasting too much material. What you want to avoid is getting glued to a flaming rag. I haven't had a problem with Hot Stuff. HS is not the only glue, but it does work well. It has a slight delay between initial and final tack. You might feel fingers get glued together at some point, and yet you can usually pull them apart I you don't wait. The same with polishing, the rag doesn't get caught if you keep moving.
As you proceed the pad hardens off. I just keep wetting it, with a drop or two, it seems to work just as well once it builds up. This obviously isn't real polishing because you can't melt into the surface. But you can keep building on it. If it starts to get rough let everything dry well and sand smooth and start up again.
If you were doing a small part that didn't catalyze, the overall approach is similar, you just have to kinda prime the piece first, possibly sand then go start up again. You may have to be a little careful as you first start since the wood will stay wet a little and possibly grab you pad. I use the same pad through though, just start out laying the primer coat.
A lot of irritating fumes will come off when doing this, so have ample fresh air.
Re: cyano-acrylate finish
John Aniano in NJ....
>Thom,
Is there a solvent that you know of that keeps CA glue thinned to better enable such a wipe-on finish?
John
Maybe...
Scott Burr in Ben Lomond CA
>Acetone would. That's what's recommended for un-sticking ones self.
Fingernail polish might work as well.
Re: cyano-acrylate finish
Wendell @ Murphy, TX
>I use CA as a finish on wooden pens I turn. I use a plastic called Delrin, cut into strips to apply the glue while the pen is spinning on the lathe. After applying the finishing, I level the finish with 320 and 400 grit sandpaper. I do the final polish using a product called Micro-Mesh. I use their pen turning finishing set which consists of 9 abrasive pads from 1500 grit up to 12,000 grit. Note that Micro-Mesh uses their own grit scale which is different than the normal sandpaper grits. I finish up with a plastic polish call Micro-Gloss that takes out the rest of the minor scratches. I've never tried the finish on flat work. I would guess that applying the CA evenly is going to be the hardest part. Micro-Mesh make the same abrasives in larger pads and even sander disks. I would also think that CA as a finish would get expensive in a hurry for articles larger than a pen. There are some pen turners that dissolve plexi-glass, i.e. acrylic in acetone to use as a finish. The resulting finish is basically the same as using CA, but I would suspect it is cheaper. You would also be able to use acetone to thin the mix which I suspect won't work with CA.
Wendell
Re: cyano-acrylate finish
ThomD
>I don't know of one. The watery stuff works great as is. But I haven't mixed up a big batch. And one is stuck using it a few drops at a time, which is actually sorta what happens with French Polish also, except there is a resevoir in the fad, which in the glue case hardens up right away.
About the largest stuff I do is bridges on guitars. If I go larger and need that kind of plastic, I probably use epoxy. A number of big name guitar folk finish with 5 minute epoxy, which blew me away. I'm talking big names. That has to be top coated if it is to see any sun. I've done fishing rods that way, but I didn't charge 5 grand for them, in fact I just used them for my own stuff, when I needed a fast job.