Thomd & Paul Kirkegard

#1

Thomd & Paul Kirkegard

Tom Colligan


>Two weeks ago I asked if anyone new what the trick was to increase the strenght of HHG. I said I know I read a prior thread but couldn't locate it via a search. William Duffield said I needed to get into Archives first and do a search from there. Well here are the posts and since neither of you participated I thought you'd like to read these especially the first one by John Aniano. I hope this works. This thread is from 11-25-05:

I was speaking the other day with my friend, the well-known NYC violinmaker James McKean, about hot hide glue. He related an observance made by an equally well-known violinmaker and restorer, William Monical. In essence it is this: hot hide glue develops it's greatest strength after it is heated thoroughly, allowed to cool thoroughly and reheated a second time. If hide glue is used to glue a wood joint while liquid from it's first heating cycle, it will not be satisfactory and will fail. Bill Monical somehow learned this "fact", told James and helped solve a number of strength issues James had had with his instruments very early on in his instrument making career.

James said that he normally makes a new batch of hot hide glue when he wants the glue joint to be as invisible as possible. Otherwise, he feels that allowing the glue to cool and stay unused for up to about a week will not make all that much difference in the strength.

At my asking, James also said that some makers did put garlic into hot hide glue and felt that of the modern NY makers doing this, they probably got the idea from Mr. Simone Sacconi, the great maker and restorer who ran the shop at the now-closed Wurlitzers in NYC.

Hope this was of interest...

John

Messages In This Thread

More Hot Hide Glue tips... (views: 278) -- John Aniano, somewhere in NJ... -- Monday, 21 November 2005, at 9:52 p.m.

Re: More Hot Hide Glue tips... (views: 214) -- Todd Stock -- Tuesday, 22 November 2005, at 11:20 a.m.

re (views: 196) -- glh -- Tuesday, 22 November 2005, at 11:32 a.m.

Good idea! *NM* (views: 74) -- Clay C in Miami -- Tuesday, 22 November 2005, at 2:45 p.m.

Re: Containers (views: 164) -- Tom Colligan, Peoria -- Tuesday, 22 November 2005, at 7:53 p.m.

Re: Containers (views: 137) -- Todd Stock -- Wednesday, 23 November 2005, at 9:28 a.m.

Re: Containers *LINK* (views: 84) -- Greg B�tit, Crown Point NY -- Wednesday, 23 November 2005, at 8:38 p.m.

Re: re (views: 152) -- danielfisherin@cs.com -- Tuesday, 22 November 2005, at 8:53 p.m.

Re: More Hot Hide Glue tips... (views: 141) -- Dick Schafer -- Wednesday, 23 November 2005, at 10:54 a.m.

Re: More Hot Hide Glue tips... (views: 82) -- Todd Stock -- Wednesday, 23 November 2005, at 10:17 p.m

Re: Thomd & Paul Kirkegard

#2

Re: Thomd & Paul Kirkegard

Paul Kierstead


>Thanks! That will make some interesting reading I bet.

I have often heard that the first heating is not as strong.

I suspect the garlic is just because ... well, not everyone cares for the smell :)

Re: Thomd & Paul Kirkegard

#3

Re: Thomd & Paul Kirkegard

thomd coralseacat@yahoo.au


>I didn't know that or can't remember it. I actually re-use the same pot over and over until something seems to go wrong with it. Not something i would recomend for a high dollar, high load application, but it shows how forgiving it can be.

Thanks!

Re: Thomd & Paul Kirkegard

#4

Re: Thomd & Paul Kirkegard

Warren in Lancaster, PA


>As Thom mentioned, hide glue is pretty forgiving. You can add glue to make it thicker, or add water if it has gotten too thick, or add both if you just want more glue. Some times you can let it sit for long periods without it going bad, depending on the temperature and how thick it is (dryer lasts longer).

When I have a particularly ticklish job, I clean out the pot, soak some glue, heat, cool and heat again. This second heating is not necessary for day to day use, but it gives the nicest texture and it spreads the nicest. I suppose I long suspected it was strongest at this time, but the way it comes off the brush and coats the surface is the reason I occasionally go to this extra trouble, and this ease of application also contributes to the quality of the work. The quality gradually decreases with subsequent heatings. The one week rule is just a guideline; when you have worked with it a lot you can judge the condition.

Garlic is a mild fungicide and antibiotic. It would discourage bacteria and mold, but probably does not add strength on its own.