Home Articles Forums Gallery Marketplace Videos

WoodCentral Forums

Knowledge You Can Build On — Est. 1998

Urban Salvaged Hardwood Slabs, Milled In-House from Rare Trees. Shop Unique Walnut Stock.

Hot Hide Glue Question

Posts

Hot Hide Glue Question

#1

Hot Hide Glue Question

Tom Colligan


>I put about an inch of granules in a quart mayo. jar and and about 5 times this amount of water and let stand for 20 hours. I planned on having to pour out the upper portion as being the excess amount of water that could not be absorbed. Yet 20 hours later there is no differential.

Was it a mistake to leave the granules in so long?

On a coffemaker I've had this syruppy gel for an hour and it's very watery now; much more so then at the start. Is it necessary to leave it at approx. 150 degrees for several hours and not just one hour? I thought that once it reaches 150 degrees or so it would then be ready, no? Tia, Tom.

Re: Hot Hide Glue Question

#2

Re: Hot Hide Glue Question

Paul Kierstead


>I think that, yes, you got much too much water in it. I normally put enough water to "cover", maybe a tad more. Once it jells up all nice, I consider it "done" and freeze or use. When I use it, it is usually too think once heated, but it is pretty easy to add a little water to make it the right consistency. If you get too much, you either let it cook for a while (water will evaporate) or perhaps mix it with some real thick stuff.

If it starts out at the right consistency, then yes it is ready when it reaches temperature. People always give some guidelines for consistency, but mostly you have to fart around to learn and gain experience.

Re: Hot Hide Glue Question

#3

Re: Hot Hide Glue Question

thomd@yahoo.au


>That's pretty much my recipee also.

Re: Hot Hide Glue Question

#4

Paul and Thom, . . .

Tom Colligan


>Thanks for your advice. I can't seem to get the search feature to work for me as I'd like to look up your input recently about upping the strength of HHG. That is, in the past 12 months someone posted what an instrument maker does to significantly strengthen the glue rather then the usual way of dealing with it.

Again, thanks for your input.

Re: Hot Hide Glue Question

#5

Re: Paul and Thom, . . .

thomd coralseacat@yahoo.au


>There are different strength grades, but the regular stuff I get form Lee Valley is very strong. It's stronger than the wood. Don't overheat, don't add glycerine.

The LMII book has the following recipee, 1.25-1 water to glue by weight, for rapid assembly, and 1.625-1 for slower assembly. Place components in a glass or plastic container for 1.5 hours until it is a gelatinous mass, then heat to no more than 150, and use.

I have a number of articles on hide glue from the luthier's point of view. Frank Ford wrote one of the better ones, so it might be worth checking his frets web site. If I knew exactly what you were after I could track something down. As long as the glue tacks well between your fingers and pulls strings, it is probablt good enough for instrument work. The strongest grades of hide glue are not made for woodwork.

Re: Hot Hide Glue Question

#6

Re: Paul and Thom, . . .

Paul Kierstead


>I'd like to look up your input recently about upping the strength of HHG.

I use 192 and 251 gram strength, and let me tell you the 251 takes some practice with; it grabs fast. Any stronger and it will be difficult to use; you'll want to make sure you want it stronger ...

Re: Hot Hide Glue Question

#7

Re: Paul and Thom, . . .

thomd coralseacat@yahoo.au


>The only part that is massively loaded is the bridge, depending on constrution. Neck and braces are neutral axis, I don't think most of the body is heavily loaded, and the neck/body attachment is not really heavily loaded though it is prone to deformation. So on the bridge you don't want something that is going to give a bad finish, the standards being as high as they are. Personally I use titebond, and if I lived in the US I would use the LMII white glue which is excellent, and hide glue on occasion. I don't like most white glues for creep. so how good does a hide glue need to be to beat white glue?

Ford mentions prefering the 192 glue. He buys 50 pound bag from the maker in Jamestown NY and stores it in bags for a lifetime supply, that way he never has batch inconsistancies.

Re: Hot Hide Glue Question

#8

Re: Hot Hide Glue Question

William Duffield, on the Cohansey


>Did you search the Hand Tool Archives as well as the current messages? After a few months, Ellis moves the old messages from the current list to the archives. To find the archived messages, instead of clicking on Search at the top of the forum page, you need to go over to the left hand side in the brown frame and click on SEARCH there, next to the blue/purple flashing spot .

As Tom notes, "Not More Than 150�" is important. If you heat it somewhat less than 150� it may be a little weaker, but if you cook it much over 150�, you will ruin it. I don't know what kind of thermostat you are using, but many of them aren't calibrated too precisely. You are better off erring on the conservative side while you are learning, until you get used to using HHG and your particular glue pot.

Re: Hot Hide Glue Question

#9

Re: Hot Hide Glue Question

Adam Cherubini,NJ


>When I add too much water, I just add more dry glue. If you think that would waste all of your glue, you have our permission to throw out this batch, but why not try it? Watery glue can be good. And it will be even better the next day. Hide glue should be watery. At least you'll know what to do next time. Just don't get too wrapped around the axle with it. Don't worry too much about the heat or water to glue ratio or any of it. If you do as I do and play dumb it all seems to work out okay. (its amazing how that glue can sense a nervous workman- almost like dog or a chisel senses fear)

Adam

Re: Hot Hide Glue Question

#10

LMII Book and LMll White Glue

Tom Colligan


>Well, Thom, I've done a google search and can not come up with anything on either. So would you advise what each is? If you'd like, I can try and get some and ship it to you. Just let me know.

Re: Hot Hide Glue Question

#11

Re: LMII Book and LMll White Glue

thomd coralseacat@yahoo.au


>Thanks.

LMII.com They used to have a luthiers catalogue with a lot of exerter info in it, may still have it. I think the Frank Ford article is probably more up to date.

They sell a white glue, the only difference it has is that it is very hard and resistant to creep. I got one bottle and really liked it. They say it has a limited shelf likfe and that is true. I just found their postage to Canada was unpredictable and often really expensive. But within the US it should be fine.

http://www.lmii.com/CartTwo/thirdproducts.asp?searchtext=glue&NameProdHeader=Instrument+makers+glue

Always use fresh white glue. White glue is sometimes better than yellow, though the Titebond luthiers seem to like is yellow, but not as thick as the yeloow cabinetmakers glue by Elmers and others. Titebond is my main workshop glue these days though I have gallons of epoxies, polys etc... For guitars i only use the Titebond and the LMII, epoxy, CA, and hide. I never try other white glues, I stick with the trade standards. Actually CA is so important for one thing or another I bet some guys might pick it over anything else if they had to make do with one kind only.

Re: Hot Hide Glue Question

#12

Re: LMII Book and LMll White Glue

Todd Stock


>The LMI white dries very hard and is a great instrument glue. Lasts about 6 months, so I buy the small containers. Great for jobs that take too long for HHG (closing bodies; fretboards, etc.).