I am late to the veneer party. I have brought my edge gluing habits with me, namely, use as little glue as will do the job and coat both surfaces, which enables using little glue.
I use a foam paint roller, a tip I got from someone that routinely veeners boxes for sale. It does not waste significant glue, it is easy to clean and reuse and it can be bagged for several days if one is veneering over several days.
I have tried brush and vee grooved card as I learned in the Headley shop. The roller is times faster, lays down an absolutely uniform film of glue and the thickness can be controlled. The panels I just finished were glued in a fraction of a minute.
To bond, both faces must be wet by the glue. If only the substrate is coated a thicker coating of glue is needed to ensure wetting of the veneer face. Because I am laying down a thin layer of glue I don't get the excessive curling I used to before the roller. Once I put substrate on veneer the thin glue layer tacks almost instantly. I don't have to worry about it skidding around before the air is pumped out. I have so little glue involved I don't expect to ever see any issue from moisture, or at least I haven't.
I am using ordinary white or yellow glue, as I learned in the Headley shop, and this glue may behave significantly different from "veneer glue". What I do may be inappropriate for thickened veneer glue. Some, maybe all, the veneer glues contain filler to increase the viscosity. I have so little glue involved that glue running here and there under vacuum is not observed.
Possibly because less glue (and water) is used the box person routinely veneers one side of 1/2" plywood with out any warping observed.