I went to Home Disappointment this morning to pick up some Titebond, expecting to see the usual TBI, TBII, and TBIII. Instead, the store offered Original, Premium, and Ultimate. Ultimate, by the way, is a white glue.
Is it just a new name on old products or new glues altogether?
Anyone have experience with the TB Ultimate white glue?
It lacks the cross linking chemistry of all the yellows. (the crosslinking is different among the yellows with regular being reversible with heat and moisture and the others not. )
I have half a big tub of it still... probably 10 years old at this point, but it seems to last forever out here. Still good last time I used some, maybe 2 years ago.
Jess, I don't use any of them for my bent laminations. I prefer epoxy for that purpose. It has a much longer open time, acts like a lubricant between parts, and sets up harder, for less creep. It also has good bridging strength, if by chance two surfaces don't make perfect contact.
If you choose one of those, go with the longest open time, if the project is large. It is heartbreaking to start bending a bundle of laminates over a form, and have the bottom plys buckle out, due to the glue having already grabbed. They don't do so well after torn apart, and moved. Epoxy on the other hand will still be good if you let it squirm even after it jells, as long as it is still making contact between parts.
Weldwood plastic resin glue - urea formaldehyde powder mixed with water. Favorite of boat builders for spar lamination. Note that color is a medium brown.
Alternatively epoxy with suitable thickeners - high density for strength and amorphous silica for viscosity increase. Add a little low density if you want a brown glue line. West System terminology used here.
Conventional wisdom says that you have to have at least 7 layers to avoid spring-back.
I've used both TBIII and plastic resin for bent lams, and in my mind there is no comparing the two - springback was pretty much nil with the resin, I forget how many lams, maybe 12 or so.
I hated mixing the stuff until I started doing it right - by weight rather than volume. Apply with one of those disposable trim paint rollers and it all goes pretty quick and easy.
I would agree with that. If we are talking the tan powder stuff. Great glue, about the third use I became spectacularly allergic to it, though I work pretty clean. But it is for sure better than most other things including epoxies which I use in most cases where I need to make stuff laminated, because it can be used in so many processes. But the tan glue is harder if you don't mind the glue line.