Re: Data you will respect
TomD
These guys have their own lab, some of their testing methods have become engineering standards. One of the borthers, Meade, is an engineer.
Unfortunately the article that deals specifically with PVC is not on the net, but the process for PVC is described in the Gluing Plastic article.
http://www.epoxyworks.com/26/pdf/Gluing_plastic_Gflex.pdf
http://www.epoxyworks.com/28/pdf/Plastic_engine_cover.pdf
http://www.epoxyworks.com/16/glueinglumber.html
http://www.epoxyworks.com/17/corian.html
"To flame treat a plasticsurface, hold a pro
-
pane torch so the flame just touches the sur
-
face and move it across the surface at a rate of
12 or 16 inches per second. Keep the torch
moving and overlap the previous pass slightly.
When done correctly, the surface will not dis
-
color or burn in any obvious way. This tech
-
nique oxidizes the surface and improves
adhesion. For best adhesion, bond to the sur
-
face within 30 minutes of treatment."