Got That
Mark Mandell - Gone Round In New Jersey
from a guy on the AAW turning forum.
Several issues:
1. You have to mix a large amount (4 liters) because the "product" is (apparently) not homogeneous in the bottle and must be used in a single mix and then allowed to sit for 3 days before use.
2. You loose the great advantage of current shellac and lacquer finishes, that being 100% burn-in for repairs.
3. They seem to want industrial grade DNA and exclude use of "hardware store" alcohols.
Since I use shellac as an intermediate step in my finishes, the advertised benefit of a more resistant film is not as important to me. The long pot life (18 months) and increased toughness would be important, especially when using toning applications, to counteract cold checking under my waterborne top coats. For me, the issues outweigh the benefits so I'll pass on the stuff but file the information for future consideration.
Thanks for the google 