a new glue 2p-10
del schisler
here is a new glue to me the link , i don't have any thing to do with the co. just thought people may neeed this type of glue,
http://www.fastcap.com/estore/pc/viewPrd.asp?idproduct=12826&idcategory=48#!prettyPhoto
Knowledge You Can Build On — Est. 1998
a new glue 2p-10
del schisler
here is a new glue to me the link , i don't have any thing to do with the co. just thought people may neeed this type of glue,
http://www.fastcap.com/estore/pc/viewPrd.asp?idproduct=12826&idcategory=48#!prettyPhoto
Re: Been using it at least 2 years...
Rick L
Certainly not new. Nexabond is certainly newer. http://www.e-zbond.com/Product.htm#Cyanoacrylate If you want quantity prices on CA Super Glue and Accellerator EZ Bond is the place to go. Even have Rubber Toughened CA. Very good source and good prices.
new to me , just some one told me dark ages?
Re: Been using it at least 2 years...
del schisler
when you spray the activator does it affect any staining process ? just wondering , thanks for a reply del
Re: Technically it's an accellerator...
Rick L
and all the accellerators I've used are acetone based. As long as you didn't get the CA glue in a spot you don't want, he accellerator won't affect anything.
clarification
Bill Tindall, E.Tn.
Anything basic sets off this polymerization(curing) reaction. The accelerator (catalyst in chemical terms) is a hindered amine which is dissolved in a fast evaporating solvent, usually acetone. The acetone flashes off leaving behind the non-volatile amine which catalyzes the cure.
The amines in the proteins in you fingers do a dandy job of catalyzing the cure, as those who have stuck a finger together know well.
to answer your question
Bill Tindall, E.Tn.
The amount of catalyst dissolved in the acetone is small. Doubtful what ever is left behind will affect any finishing. That said, some of the conversion varnishes are acid catalyzed. Still, I don't think a typical spritz of catalyst would be enough to effect finish.
thanks Bill
Re: a new glue 2p-10
Larry Clinton At Frankfort, (Central) Indiana
This appears to me to be a run of the mill Cyanoacrylate Adhesive, I used many gallons of this type adhesive in my old job as an Engineer. The products we used were of 3M manufacture. I use the same products in my shop for certain applications, mostly for filling small imperfections in the surface of wood - a small amount of superglue and sawdust from the sander works pretty well and seems to stain and finish without problems. I have also used it to replace a "splinter" but normally just use Titebond unless I am in a hurry or if would be extremely hard to "clamp" the parts.
It is unusual (at least in my experience) to require an accelerator for normal cure. I have used accelerators - but only to speed up the cure. Normally there is enough moisture in the air or substrate to polymerize the glue. In our industrial applications we dispensed by spray, drops and in certain cases with a brush, but never used an accelerator.