This article lives on
Bill Tindall, E.Tn.
Spencer and I wrote it years ago for WoodCentral or Badger Pond, I don't remember which. A German woodworker asked if he could post it at some museum web site. From there it seems to have propagated far and wide.
Every few months we get an email concerning the article. Usually it is some shrill environmentalist railing that we have recommended despoiling the environment through generation of chromate when the preferred stainless steel anodes are used. Somewhere back in time someone made the claim that stainless steel will generate chromate when used as an anode in this cleaning. As is usually the case these folks have lots of concerns and little technical knowledge. I have asked each time for a reference to where this claim came from but so far no data has been produced to substantiate it.
A biochemistry graduate student (no doubt from CA)was particularly aggressive and was going to have us arrested if we did not retract the stainless steel recommendation at once. He was entertaining to engage. A degree in biochemistry does not leave one prepared to argue the details of this chemistry. He was unable to provide any citations to support his claims. I hope he did better in his thesis defense.
A friend has a 55 gallon electrolysis bath which has a stainless steel screen for an anode. I had this solution analyzed and found it contained around 1 part per million of chromium in some form or another. The amount was too piddly to be concerned with the details of what form the chromium was in. Another critic wedded to the chromate belief argued that the solution had been analyzed incorrectly and that was the reason no chromate was found in significant amounts. He did not fair well either in the exchange.
As a point of fact a 304 stainless steel anode will suffer only slight attack when used as an anode. What ever tiny amount of chromium might be removed will most likely wind up as harmless chromium hydroxide in the bottom of the bath. It will join the environment along with the hundreds of pounds of stainless steel being dissolved each year through corrosion of the local chemical plants.
There are many kinds of stainless steel. It may be that one of the less corrosion resistant varieties could generate small amounts of chromate at the anode. However, lots of stuff that would turn chromate into a benign form of chromium will be present in the bath. So, in the absence of data to the contrary I don't believe chromate generation should be a concern when using a stainless steel anode. No doubt those that make a career about fretting will continue to do so and we will continue to get emails.
Should one be concerned about the toxicity stuff being generated in the bath then focus on other factors. Paint pigments in days past contained cadmium and lead. If rebar is used it is made from recycled metal and it does dissolve releasing what ever might be there which will surely include chromium, etc.
I have been emailed about using the process to derust tractors. Just yesterday I was asked about details of attaching the anode by an exceptionally polite responder who was provided a detailed answer.